Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsamid® AESNO P401 TL - PA12 - ARKEMA

Material Data Center offers the following functions for Rilsamid® AESNO P401 TL:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Rilsamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
ISO 16396 - PA12-P, EGHL, C22-004

Rilsamid® AESNO P401 TL resin is a natural polyamide. 
This grade is plasticized and designed for tube extrusion.

Rilsamid® AESNO P401 TL resin falls into the PA12-HIPHL category according to DIN 73378.


Main applications:

Tubings

Packaging:
This grade is delivered dried in sealed packaging (44 lb bags / 1000 lb containers) ready to be processed.

Shelf life:
Two years from the date of delivery. for any use above this limit, please refer to our technical services.
Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 13 / * cm³/10min ISO 1133
Temperatura 235 / * °C -
Carga 5 / * kg -
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción - / 360 MPa ISO 527
Esfuerzo a 50% de alarg. - / 24 MPa ISO 527
Alargamiento a rotura - / >50 % ISO 527
Resistencia al impacto Charpy c/entalla, +23°C 46 / - kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 4 / 8 kJ/m² ISO 179/1eA
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 174 / * °C ISO 11357-1/-3
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Resistencia dieléctrica 41 / - kV/mm IEC 60243-1
Indice comparativo de linea de fuga 600 / - - IEC 60112
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 1.2 / * % Sim. to ISO 62
Densidad 1030 / - kg/m³ ISO 1183
Recomendación para procesamiento ExtrusiónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 80 °C -
Tiempo de pre-secado 4 - 6 h -
Temperatura de la masa 230 - 270 °C -
Características
Procesamiento y forma de entrega
Extrusión de tubería
Aditivos
Plastificante
Disponibilidad regional
Demás información
Otros tipos de extrusión

Processing conditions for extrusion :

- Typical melt temperature (Min / Recommended / Max) : 230°C / 250°C / 270°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 80°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.