Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® MB 3610 NAT - PA11-I - ARKEMA

Material Data Center offers the following functions for Rilsan® MB 3610 NAT:
unit conversion, PDF datasheet print, comparison with other plastics, parameters for material models, CAE Interfaces

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
PA11-P, EHL, 22-002
Rilsan® MB 3610 NAT resin is a polyamide 11 produced from a renewable source. This natural grade is plasticized and specially designed for pneumatic applications. It combines very high flexibility with good impact resistance.



Main applications:
  • Pneumatic tubing

Packaging:
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 4 / * cm³/10min ISO 1133
Temperatura 235 / * °C -
Carga 5 / * kg -
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción - / 210 MPa ISO 527
Resistencia al impacto Charpy c/entalla, -30°C - / 10 kJ/m² ISO 179/1eA
Dureza Shore D 53 / * - ISO 7619-1
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 188 / * °C ISO 11357-1/-3
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Resistividad volumétrica específica 1.9E11 / - Ohm*m IEC 62631-3-1
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 1.1 / * % Sim. to ISO 62
Absorción de humedad 0.45 / * % Sim. to ISO 62
Densidad 1030 / 1030 kg/m³ ISO 1183
Biobased content 59 % -
Funciones
Viscosidad-velocidad de cizallamiento , Rilsan® MB 3610 NAT, PA11-I, ARKEMA
Tensión de cizalla-velocidad de cizalla , Rilsan® MB 3610 NAT, PA11-I, ARKEMA
Esfuerzo-alargamiento , Rilsan® MB 3610 NAT (Seco), PA11-I, ARKEMA
Módulo secante-alargamiento , Rilsan® MB 3610 NAT (Seco), PA11-I, ARKEMA
Características
Procesamiento y forma de entrega
Extrusión de perfiles
Forma de suministro
Sémola, Color natural
Aditivos
Plastificante
Características especiales
Alto impacto o modificado al impacto, Estable a la luz, Estable contra rayos U.V./interperie, Estable contra el calor
Certifications
Contiene recursos renovables
Disponibilidad regional
Demás información
Otros tipos de extrusión

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 230°C / 250°C / 280°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-8 hours at 80-90°C.

Resistencia a medios químicos
Acidos
Ácido acético (5% por masa) (23°C)
Solución ácido cítrico (10% por masa) (23°C)
Ácido láctico (10% por masa) (23°C)
Ácido clorhídrico (36% por masa) (23°C)
Ácido nítrico (40% por masa) (23°C)
Ácido sulfúrico (38% por masa) (23°C)
Ácido sulfúrico (5% por masa) (23°C)
Solución ácido crómico (40% por masa) (23°C)
Bases
Solución de hidróxido de sodio (35% por masa) (23°C)
Solución de hidróxido de sodio (1% por masa) (23°C)
Solución de hidróxido de amónio (10% por masa) (23°C)
Alcoholes
Metanol (23°C)
Etanol (23°C)
Hidrocarburos
N-hexano (23°C)
Tolueno (23°C)
Cetonas
Acetona (23°C)
Aceites minerales
SAE 10w40 aceite motor multigrado (23°C)
SAE 10w40 aceite motor multigrado (130°C)
SAE 80/90 aceite para engranajes hipocíclicos (130°C)
Aceite aislante (23°C)
Combustibles normales
ISO 1817 líquido 1 (60°C)
ISO 1817 líquido 2 (60°C)
ISO 1817 líquido 3 (60°C)
ISO 1817 líquido 4 (60°C)
Combustible normal sin alcohol (pref. ISO 1817 líquido C) (23°C)
Combustible normal con alcohol (pref. ISO 1817 líquido 4) (23°C)
Combustible diesel (pref. ISO 1817 líquido F) (23°C)
Combustible diesel (pref. ISO 1817 líquido F) (90°C)
Combustible diesel (pref. ISO 1817 líquido F) (>90°C)
Soluciones de sal
Solución de cloruro de sodio (10% por masa) (23°C)
Solución de hipoclorito de sodio (10% por masa) (23°C)
Solución de cloruro de cinc (50% por masa) (23°C)
Otros
Acetato etílico (23°C)
Agua oxigenada (23°C)
Fluido de freno DOT no. 4 (130°C)
Glicol etilénico (50% por masa) en agua (108°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.