Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Spectar™ - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Spectar™:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Spectar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

Eastman Spectar™ Clear is a copolyester, developed by Eastman to achieve measurably improved sheet clarity and edge color while maintaining the performance characteristics for which Eastman Spectar™ copolyester has become known in the industry. It offers the thermoformability and ease of fabrication of Eastman Spectar™ copolyester along with significantly improved clarity. Eastman Spectar™ Clear also offers approximately double the notch impact strength, 50% higher instrumented impact strength and better chemical resistance when compared

to traditional Spectar™ Copolyester.




Propiedades mecánicasValorUnidadesMétodo de ensayo
ASTM Data
Módulo de tracción 1800 MPa ASTM D 638
Esfuerzo de fluencia a tracción 48 MPa ASTM D 638
Esfuerzo de fractura a tracción 53 MPa ASTM D 638
Alargamiento a la fluencia 5 % ASTM D 638
Alargamiento a la rotura 340 % ASTM D 638
Módulo de flexión 2000 MPa ASTM D 790
Dureza Rockwell R 107 - ASTM D 785
Resistencia al impacto Izod con entalla, 1/8 in N J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 83 J/m ASTM D 256
Temperatura -30 °C -
Resistencia al impacto Izod, 1/8 in N J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ASTM Data
Combustibilidad UL 94 HB - UL 94
Coeficiente de dilatación térmica, long. 76.2 E-6/K ASTM D 696
Estabilidad al calor @ 66 psi 77 °C ASTM D 648
Estabilidad al calor @ 264 psi 73 °C ASTM D 648
Temperatura Vicat 86 °C ASTM D 1525
Propiedades eléctricasValorUnidadesMétodo de ensayo
ASTM Data
Resistividad superficial 1E17 Ohm ASTM D 257
Resistividad volumétrica 1E16 Ohm*cm ASTM D 257
Resistencia al arco 130 s ASTM D 495
Propiedades opticasValorUnidadesMétodo de ensayo
ASTM Data
Brillo 150 - ASTM D 2457
Opacidad 0.5 % ASTM D 1003
Transmitancia luminosa 91 % ASTM D 1003
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua, 24hr 0.19 % ASTM D 570
Densidad 1230 kg/m³ ASTM D 792
Características
Procesamiento y forma de entrega
Extrusión de láminas, Termoconformación
Características especiales
Alto impacto o modificado al impacto, Transparente
Características
Bajo olor, Copolímero
Resistencia quimica
Resistencia química general
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.