Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Styrolution® PS 168N - PS - INEOS Styrolution

Material Data Center offers the following functions for Styrolution® PS 168N:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Styrolution PS datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Styrolution® PS 168N is a high molecular, heat resistant grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. As blend component with high impact Polystyrol or Styrolux.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 1.5 cm³/10min ISO 1133
Temperatura 200 °C -
Carga 5 kg -
Densidad de fusión 936 kg/m³ -
Conductibilidad termica de fusión 0.155 W/(m K) -
Calor especifico de la masa 2300 J/(kg K) -
Temperatura de expulsión 96 °C -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 3300 MPa ISO 527
Resistencia a la tracción 59 MPa ISO 527
Alargamiento a rotura 3 % ISO 527
Módulo de plastodeformación, 1h 3300 MPa ISO 899-1
Módulo de plastodeformación, 1000h 2600 MPa ISO 899-1
Resistencia al impacto Charpy c/entalla, +23°C 4 kJ/m² ISO 179/1eA
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temp. de transición vítrea, 10°C/min 100 °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 86 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 98 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 101 °C ISO 306
Coef.de expansión térmica lineal, paralelo 80 E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB class IEC 60695-11-10
Espesores de probeta 1.5 mm -
Yellow Card disponible - -
Combustibilidad a espesor h HB class IEC 60695-11-10
Espesores de probeta 3.2 mm -
Yellow Card disponible - -
Combustibilidad según índice de oxigeno 18 % ISO 4589-1/-2
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 2.5 - IEC 62631-2-1
Constante dieléctrica, 1MHz 2.5 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 0.9 E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 0.5 E-4 IEC 62631-2-1
Indice comparativo de linea de fuga 475 - IEC 60112
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1050 kg/m³ ISO 1183
Propiedades específicas del materialValorUnidadesMétodo de ensayo
ISO Data
Indice de viscosidad 119 cm³/g ISO 307, 1157, 1628
Condiciones de transformaciónValorUnidadesMétodo de ensayo
ISO Data
Moldeo por inyección, temperatura de la masa 230 °C ISO 294
Moldeo por inyección, temperatura del molde 40 °C ISO 294
Moldeo por inyección, velocidad de inyección 200 mm/s ISO 294
Funciones
Viscosidad-velocidad de cizallamiento , Styrolution® PS 168N, PS, INEOS Styrolution
Tensión de cizalla-velocidad de cizalla , Styrolution® PS 168N, PS, INEOS Styrolution
Esfuerzo-alargamiento , Styrolution® PS 168N, PS, INEOS Styrolution
Módulo secante-alargamiento , Styrolution® PS 168N, PS, INEOS Styrolution
Esfuerzo-alargamiento (isocrono) 23°C, Styrolution® PS 168N, PS, INEOS Styrolution
Módulo de plastodeformación-tiempo 23°C, Styrolution® PS 168N, PS, INEOS Styrolution
Curva de creep 23°C, Styrolution® PS 168N, PS, INEOS Styrolution
Volumen especifico-temperatura (pvT) , Styrolution® PS 168N, PS, INEOS Styrolution
Módulo a tensión-temperatura , Styrolution® PS 168N, PS, INEOS Styrolution
Características
Procesamiento y forma de entrega
Moldeo por inyección, Extrusion del film, Extrusión de perfiles, Extrusión de láminas, Otros tipos de extrusión
Forma de suministro
Sémola
Características especiales
Transparente
Disponibilidad regional
Demás información
Moldeo por inyección
PROCESSING
injection molding, Melt temperature, range: 180 - 280 °C
injection molding, Melt temperature, recommended: 230 °C
injection molding, Mold temperature, range: 10 - 60 °C
injection molding, Mold temperature, recommended: 40 °C

Polystyrol 168N can be injection molded at temperatures between 180 and 280°C.Recommended mold temperatures are between 10 and 60°C.
Extrusión de láminas
PROCESSING
Extrusion, Blown film, Melt temperature: 190 - 220 °C
Extrusion, Flat film, Melt temperature: 210 - 240 °C

Extrusion melt temperature should not exceed 240°C.
Otros tipos de extrusión
PROCESSING
Extrusion, Pipes, Melt temperature: 180 - 220 °C
Extrusión de perfiles
PROCESSING
Extrusion, Profiles, Melt temperature: 220 °C
Extrusión de placas
PROCESSING
Extrusion, Plates, Melt temperature: 210 - 240 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.