Caracteristicas de procesamiento y fisicas | Valor | Unidades | Método de ensayo |
Other Standards[S] |
Índice de fluidez, MFI |
8 |
g/10min |
ASTM D 3307 |
Temperatura |
372 |
°C |
- |
Carga |
5 |
kg |
- |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propiedades mecánicas | Valor | Unidades | Método de ensayo |
Other Standards[S] |
Esfuerzo de tracción |
28 |
MPa |
ASTM D 3307 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propiedades térmicas | Valor | Unidades | Método de ensayo |
Other Standards[S] |
Temperatura de fusión |
285 |
°C |
ASTM D 4591 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propiedades eléctricas | Valor | Unidades | Método de ensayo |
Other Standards[S] |
Resistividad volumétrica específica |
0.11 |
Ohm*m |
ISO 3915 |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Otras propiedades | Valor | Unidades | Método de ensayo |
Densidad |
2150 |
kg/m³ |
ASTM D 792 |
Características
Procesamiento y forma de entrega
Otros tipos de extrusión, Moldeo por soplado, Transfer Molding, Moldeo por compresión
Forma de suministro
Sémola
Características especiales
Antiestático, Estable contra rayos U.V./interperie
Características
Resistencia a la fluencia, Resistencia del fundido, Estabilidad térmica, Grado tribológico
Resistencia quimica
Resistencia química general, Resistencia a solventes
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com