Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of TENAC™ MG210 - POM - Asahi Kasei

Material Data Center offers the following functions for TENAC™ MG210:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Tenac datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 1.5 cm³/10min ISO 1133
Temperatura 190 °C -
Carga 2.16 kg -
Índice de fluidez, MFI 1.7 g/10min ISO 1133
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 3150 MPa ISO 527
Esfuerzo de fluencia 75 MPa ISO 527
Alargamiento a rotura 40 % ISO 527
Módulo de flexión, 23°C 2900 MPa ISO 178
Resistencia al impacto Charpy c/entalla, +23°C 10 kJ/m² ISO 179/1eA
ASTM Data
Esfuerzo de tracción 79 MPa ASTM D 638
Alargamiento a la rotura 40 % ASTM D 638
Módulo de flexión 3040 MPa ASTM D 790
Resistencia a la flexión 108 MPa ASTM D 790
Dureza Rockwell R 120 - ASTM D 785
Resistencia a la abrasión (Taber) 13 mg/1000 cycles ASTM D 1044
Resistencia al impacto Izod con entalla, 1/8 in 78 J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 103 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 167 °C ISO 75-1/-2
Coef.de expansión térmica lineal, paralelo 100 E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB class IEC 60695-11-10
Combustibilidad a espesor h HB class IEC 60695-11-10
Espesores de probeta 0.8 mm -
Yellow Card disponible - -
ASTM Data
Coeficiente de dilatación térmica, long. 100 E-6/K ASTM D 696
Estabilidad al calor @ 66 psi 172 °C ASTM D 648
Estabilidad al calor @ 264 psi 136 °C ASTM D 648
Propiedades eléctricasValorUnidadesMétodo de ensayo
ASTM Data
Resistencia dieléctrica, tiempo corto 18 kV/mm ASTM D 149
Resistividad superficial 1E17 Ohm ASTM D 257
Resistividad volumétrica 1E16 Ohm*cm ASTM D 257
Resistencia al arco 250 s ASTM D 495
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1420 kg/m³ ISO 1183
Absorción de agua, 24hr 0.2 % ASTM D 570
Densidad 1420 kg/m³ ASTM D 792
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 80 - 90 °C -
Tiempo de pre-secado 3 - 4 h -
Temperatura de la masa 190 - 210 °C -
Temperatura del molde 60 °C -
Funciones
Esfuerzo-alargamiento , TENAC™ MG210, POM, Asahi Kasei
Módulo secante-alargamiento , TENAC™ MG210, POM, Asahi Kasei
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Características
Homopolímero
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.