Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultraform® N2200 G53 AT - POM-GF25 - BASF

Material Data Center offers the following functions for Ultraform® N2200 G53 AT:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultraform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Injection molding grade for parts requiring high stiffness and strength together with good mold release.

Abbreviated designation according to ISO 1043: POM-GF25
Designation according to ISO 29988-POM-K,GF25,M-GNR,2-3
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 3.7 cm³/10min ISO 1133
Temperatura 190 °C -
Carga 2.16 kg -
Contracción posterior al moldeo, paralelo 0.5 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 1.0 % ISO 294-4, 2577
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 9300 MPa ISO 527
Resistencia a la tracción 135 MPa ISO 527
Alargamiento a rotura 2.5 % ISO 527
Módulo de plastodeformación, 1h 7500 MPa ISO 899-1
Resistencia al impacto Charpy, +23°C 45 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C 50 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 9 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 9 kJ/m² ISO 179/1eA
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 165 °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 163 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 165 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 160 °C ISO 306
Coef.de expansión térmica lineal, paralelo 40 E-6/K ISO 11359-1/-2
Yellow Card disponible - -
Combustibilidad a espesor h HB class IEC 60695-11-10
Espesores de probeta 0.8 mm -
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 4 - IEC 62631-2-1
Constante dieléctrica, 1MHz 4 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 40 E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 70 E-4 IEC 62631-2-1
Resistividad volumétrica específica 1E10 Ohm*m IEC 62631-3-1
Resistividad superficial específica 1E14 Ohm IEC 62631-3-2
Resistencia dieléctrica 43 kV/mm IEC 60243-1
Indice comparativo de linea de fuga 600 - IEC 60112
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 1.1 % Sim. to ISO 62
Absorción de humedad 0.2 % Sim. to ISO 62
Densidad 1590 kg/m³ ISO 1183
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 100 °C -
Tiempo de pre-secado 3 h -
Humedad de procesamiento ≤0.2 % -
Temperatura de la masa 190 - 220 °C -
Temperatura del molde 60 - 120 °C -
Funciones
Viscosidad-velocidad de cizallamiento , Ultraform® N2200 G53 AT, POM-GF25, BASF
Tensión de cizalla-velocidad de cizalla , Ultraform® N2200 G53 AT, POM-GF25, BASF
Módulo de cizallamiento dinámico-temperatura , Ultraform® N2200 G53 AT, POM-GF25, BASF
Esfuerzo-alargamiento , Ultraform® N2200 G53 AT, POM-GF25, BASF
Módulo secante-alargamiento , Ultraform® N2200 G53 AT, POM-GF25, BASF
Esfuerzo-alargamiento (isocrono) 23°C, Ultraform® N2200 G53 AT, POM-GF25, BASF
Módulo de plastodeformación-tiempo 23°C, Ultraform® N2200 G53 AT, POM-GF25, BASF
Curva de creep 23°C, Ultraform® N2200 G53 AT, POM-GF25, BASF
Esfuerzo-alargamiento (isocrono) 80°C, Ultraform® N2200 G53 AT, POM-GF25, BASF
Módulo de plastodeformación-tiempo 80°C, Ultraform® N2200 G53 AT, POM-GF25, BASF
Curva de creep 80°C, Ultraform® N2200 G53 AT, POM-GF25, BASF
Volumen especifico-temperatura (pvT) , Ultraform® N2200 G53 AT, POM-GF25, BASF
Módulo a tensión-temperatura , Ultraform® N2200 G53 AT, POM-GF25, BASF
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Aditivos
Desmoldeante
Características
Copolímero
Disponibilidad regional
Demás información
Moldeo por inyección
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
injection molding, Melt temperature, range: 190 - 220 °C
injection molding, Melt temperature, recommended: 210 °C
injection molding, Mold temperature, range: 60 - 120 °C
injection molding, Mold temperature, recommended: 100 °C
injection molding, Dwell time, thermoplastics: 10 min

Processing

Usual single-flighted three-section screws with an effective screw length of at least 15 D, better 20 - 23 D are suitable for the injection molding of Ultraform.

Pretreatment

Granules or pellets in original packaging can be processed without any special pretreatment. Granules or pellets which have become moist due to prolonged or incorrect storage (e.g. by formation of condensed water) must be dried in dehumidifying or recirculating air dryers for approx. 3 hours at about 100 - 110 °C. The moisture content should not exceed 0.2 %.


Postprocessing

If parts were produced at a comparatively low mold temperature (e.g. in order to obtain short cycle times) and must not change their geometry in use thermal postprocessing inducing dimensional changes by postcrystallization may be necessary. In such cases parts should be stored in an oven with recirculated air at temperatures of 100 - 130 °C until dimensions don't change significantly any further. The time needed for this has to be determined experimentally.
Resistencia a medios químicos
Acidos
Ácido acético (5% por masa) (23°C)
Ácido láctico (10% por masa) (23°C)
Ácido clorhídrico (36% por masa) (23°C)
Ácido nítrico (40% por masa) (23°C)
Ácido sulfúrico (38% por masa) (23°C)
Ácido sulfúrico (5% por masa) (23°C)
Solución ácido crómico (40% por masa) (23°C)
Bases
Solución de hidróxido de sodio (35% por masa) (23°C)
Solución de hidróxido de sodio (1% por masa) (23°C)
Solución de hidróxido de amónio (10% por masa) (23°C)
Alcoholes
Alcohol isopropílico (23°C)
Metanol (23°C)
Etanol (23°C)
Hidrocarburos
N-hexano (23°C)
Tolueno (23°C)
Iso-octano (23°C)
Cetonas
Acetona (23°C)
Éteres
Dietil éter (23°C)
Aceites minerales
SAE 10w40 aceite motor multigrado (130°C)
SAE 80/90 aceite para engranajes hipocíclicos (130°C)
Combustibles normales
ISO 1817 líquido 1 (60°C)
ISO 1817 líquido 2 (60°C)
ISO 1817 líquido 3 (60°C)
ISO 1817 líquido 4 (60°C)
Combustible normal sin alcohol (pref. ISO 1817 líquido C) (23°C)
Combustible normal con alcohol (pref. ISO 1817 líquido 4) (23°C)
Combustible diesel (pref. ISO 1817 líquido F) (23°C)
Combustible diesel (pref. ISO 1817 líquido F) (>90°C)
Soluciones de sal
Solución de cloruro de sodio (10% por masa) (23°C)
Solución de hipoclorito de sodio (10% por masa) (23°C)
Solución de carbonato sódico (20% por masa) (23°C)
Solución de carbonato sódico (2% por masa) (23°C)
Otros
Acetato etílico (23°C)
Agua oxigenada (23°C)
Fluido de freno DOT no. 4 (130°C)
Glicol etilénico (50% por masa) en agua (108°C)
50% ácido oleico + 50% aceite de oliva (23°C)
Agua (23°C)
Agua desionizada (90°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.