Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse Z PCTG - Copolyester-Z - BASF

Material Data Center offers the following functions for Ultrafuse Z PCTG:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 67.5 cm³/10min ISO 1133
Temperatura 275 °C -
Carga 5 kg -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temp. de transición vítrea, 10°C/min 81 °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 69 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 73 °C ISO 75-1/-2
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1200 kg/m³ ISO 1183
3D DataValorUnidadesMétodo de ensayo
Other Standards[S]
Módulo de tracción, flat 1760 MPa ISO 527
Módulo de tracción, upright 1670 MPa ISO 527
Esfuerzo de tracción, flat 37.1 MPa ISO 527
Esfuerzo de tracción, upright 13.6 MPa ISO 527
Alargamiento a rotura, flat 3.1 % ISO 527
Alargamiento a rotura, upright 0.8 % ISO 527
Módulo de flexión, flat 1610 MPa ISO 178
Módulo de flexión, on-edge 1780 MPa ISO 178
Módulo de flexión, upright 1490 MPa ISO 178
Resistencia a la flexión, flat 55.5 MPa ISO 178
Resistencia a la flexión, on-edge 70.8 MPa ISO 178
Resistencia a la flexión, upright 20.2 MPa ISO 178
Resistencia al impacto Charpy, +23°C, on-edge 9.5 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C, flat 2.1 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, +23°C, on-edge 2.6 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, +23°C, upright 0.9 kJ/m² ISO 179/1eA
Resistencia al impacto Izod, +23°C, flat 14.3 kJ/m² ISO 180/1U
Resistencia al impacto Izod, +23°C, on-edge 24.2 kJ/m² ISO 180/1U
Resistencia al impacto Izod, +23°C, upright 3.4 kJ/m² ISO 180/1U
Resistencia al impacto Izod con entalla, +23°C, on-edge 3.4 kJ/m² ISO 180/1A
Resistividad volumétrica específica, flat 40000 Ohm*m IEC 62631-3-1
Resistividad volumétrica específica, on-edge 130 Ohm*m IEC 62631-3-1
S: These properties are reported by the producer according standards that are different to our defaults.
Características
Procesamiento y forma de entrega
Additive Manufacturing
Forma de suministro
Monofilamento, Negro
Características
Amorfo
Applicaciones
Electrica
Disponibilidad regional
Norteamérica, Europa, América del Sur y Centroaméric
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.