Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrasint PA6 FR black - PA6 - BASF

Material Data Center offers the following functions for Ultrasint PA6 FR black:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrasint datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 10 / * cm³/10min ISO 1133
Temperatura 240 / * °C -
Carga 2.16 / * kg -
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 218 / * °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 113 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 207 / * °C ISO 75-1/-2
Temp. reblandecimiento Vicat, A 214 / * °C ISO 306
Temp. reblandecimiento Vicat, B 197 / * °C ISO 306
Combustibilidad a espesor h V-2 / * class IEC 60695-11-10
Espesores de probeta 0.8 / * mm -
Glow Wire Flammability Index (GWFI) 750 °C IEC 60695-2-12
GWFI - thickness tested (1) 1 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.6 mm -
Glow Wire Ignition Temperature (GWIT) 775 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Densidad 1300 / - kg/m³ ISO 1183
Bulk density 550 kg/m³ -
3D DataSeco / CondUnidadesMétodo de ensayo
Other Standards[S]
Módulo de tracción, flat 4750 / 2450 MPa ISO 527
Módulo de tracción, upright 4500 / 2450 MPa ISO 527
Esfuerzo de tracción, flat 56 / 41 MPa ISO 527
Esfuerzo de tracción, upright 33 / 27 MPa ISO 527
Alargamiento a rotura, flat 1.4 / 2.6 % ISO 527
Alargamiento a rotura, upright 0.8 / 1.2 % ISO 527
Módulo de flexión, flat 4400 / 2000 MPa ISO 178
Módulo de flexión, upright 3850 / 2050 MPa ISO 178
Resistencia al impacto Charpy, +23°C, flat 4.8 / 7.4 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, +23°C, upright 2.5 / 3.6 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C, flat 1.3 / 1.6 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, +23°C, upright 1 / 1.1 kJ/m² ISO 179/1eA
Resistencia al impacto Izod, +23°C, flat 5 / 7 kJ/m² ISO 180/1U
Resistencia al impacto Izod, +23°C, upright 3.4 / 3.8 kJ/m² ISO 180/1U
Resistencia al impacto Izod con entalla, +23°C, flat 1.8 / 2.1 kJ/m² ISO 180/1A
Resistencia al impacto Izod con entalla, +23°C, upright 1.5 / 1.5 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
Características
Procesamiento y forma de entrega
Additive Manufacturing, Sinterizado por láser
Forma de suministro
Polvo, Negro
Características especiales
Resistencia mejorada al fuego
Características
Estabilidad térmica
Applicaciones
Avión y aeroespacial, Automotriz, Electrica
Disponibilidad regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.