Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Utec® 6541 - (PE-UHMW) - Braskem

Material Data Center offers the following functions for Utec® 6541:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Utec datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Esfuerzo de fluencia 17 MPa ISO 527
Resistencia a la tracción 30 MPa ISO 527
Alargamiento a rotura 350 % ISO 527
Resistencia al impacto Charpy, +23°C 100 kJ/m² ISO 179/1eU
Dureza Shore D 64 - ISO 7619-1
ASTM Data
Esfuerzo de fluencia a tracción 17 MPa ASTM D 638
Esfuerzo de fractura a tracción 30 MPa ASTM D 638
Alargamiento a la rotura 300 % ASTM D 638
Dureza D Shore 64 - ASTM D 2240
Resistencia al impacto Izod con entalla, 1/8 in N J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temp. reblandecimiento Vicat, A 128 °C ISO 306
ASTM Data
Coeficiente de dilatación térmica, long. 150 E-6/K ASTM D 696
Estabilidad al calor @ 66 psi 79 °C ASTM D 648
Estabilidad al calor @ 264 psi 48 °C ASTM D 648
Temperatura de fusión 133 °C ASTM D 3418
Conductividad térmica, estado sólido 0.0577 W/(m K) ASTM C 177
Propiedades eléctricasValorUnidadesMétodo de ensayo
ASTM Data
Resistencia dieléctrica, tiempo corto 90 kV/mm ASTM D 149
Resistividad superficial 1E12 Ohm ASTM D 257
Resistividad volumétrica 1E14 Ohm*cm ASTM D 257
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua, 24hr 0.01 % ASTM D 570
Densidad 925 kg/m³ ASTM D 792
Viscosidad intrínseca 28 dl/g -
Bulk Density 450 kg/m³ -
Características
Procesamiento y forma de entrega
Extrusión de perfiles, Moldeo por compresión
Características especiales
Alto impacto o modificado al impacto
Características
Grado tribológico
Certifications
Contacto con alimentos, Aprobado por el FDA 21 CFR
Disponibilidad regional
Norteamérica, Europa, América del Sur y Centroaméric
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.