Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VECTRA® MT®1305 - LCP-GF15 - Celanese

Material Data Center offers the following functions for VECTRA® MT®1305:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vectra datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Vectra® MT1305 VF3001 (natural) is a 15% glass reinforced, easy flow LCP grade for injection molding.

Vectra® MT1305 VF3001 (natural) is a special grade developed for medical industry applications and complies with:
  • Food Contact Substance Notification (FCN) No. 742 of the Food and Drug Administration (FDA) and is listed in the Drug Master File (DMF 8464) and the Device Master File (MAF 315)
  • the corresponding EU and national registry regulatory requirements
  • biocompatibility in tests corresponding to USP 23 Class VI/ISO 10993
  • low residual monomers
  • no animal products
Provides easier flow than MT1310 VF3001 (natural)
Slightly tougher, but may warp slightly more than MT1310 in some parts 
Chemical abbreviation according to ISO 1043-1 : LCP
Inherently flame retardant
UL-Listing V-0 in natural and black at 0.44mm thickness per UL 94 flame testing. Relative-Temperature-Index (RTI) according to UL 746B: electricals 240°C, mechanicals 220°C at 0.85mm. UL = Underwriters Laboratories (USA)

Flammability at thickness hV-0-
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Contracción posterior al moldeo, paralelo 0.1 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.4 % ISO 294-4, 2577
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 12000 MPa ISO 527
Resistencia a la tracción 190 MPa ISO 527
Alargamiento a rotura 3 % ISO 527
Resistencia al impacto Charpy c/entalla, +23°C 80 kJ/m² ISO 179/1eA
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 280 °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 230 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 250 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 162 °C ISO 306
Coef.de expansión térmica lineal, paralelo 10 E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 18 E-6/K ISO 11359-1/-2
Combustibilidad a espesor h V-0 class IEC 60695-11-10
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 3.5 - IEC 62631-2-1
Constante dieléctrica, 1MHz 3 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 200 E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 180 E-4 IEC 62631-2-1
Resistividad volumétrica específica 1E13 Ohm*m IEC 62631-3-1
Resistividad superficial específica >1E15 Ohm IEC 62631-3-2
Resistencia dieléctrica 34 kV/mm IEC 60243-1
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1500 kg/m³ ISO 1183
Funciones
Esfuerzo-alargamiento , VECTRA® MT®1305, LCP-GF15, Celanese
Módulo secante-alargamiento , VECTRA® MT®1305, LCP-GF15, Celanese
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola, Negro, Color natural
Características especiales
Resistencia mejorada al fuego, Estable a la luz, Estable contra rayos U.V./interperie, Estable contra el calor
Certifications
Food contact notification (FCN), USP Class VI, Drug Master File, Device Master File
Applicaciones
Médico
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Demás información
Moldeo por inyección
Vectra resins are well known for their excellent thermal and hydrolytic stability. In order to ensure these properties are optimum, the resin should be dried correctly prior to processing. The Vectra MT-grades MT1300, MT1305, MT1310, MT1335, MT1340 and MT1345 should be dried at 150°C for a minimum of 4 hours in a desiccant dryer.
A three-zone screw evenly divided into feed, compression, and metering zones is preferred. A higher percentage of feed flights may be needed for smaller machines: 1/2 feed, 1/4 compression, 1/4 metering.

Vectra LCPs are shear thinning, their melt viscosity decreases quickly as shear rate increases. For parts that are difficult to fill, the molder can increase the injection velocity to improve melt flow.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.