Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® Care ME47 - TPA - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® Care ME47:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Polyamide 12 elastomer molding compounds

VESTAMID® Care ME47 is free of plasticizers and heat and light stabilized. VESTAMID® Care ME47 is resistant to body fluids and toxicologically safe.

VESTAMID® Care ME grades are flexible polyether block amides (PEBA) resins.

The advantages at a glance:
  • High flexibility & elasticity
  • Good rebound properties
  • High impact resistance
  • Excellent dimensional stability
  • High chemical resistance
  • Easy processability & colorability
  • Plasticizer-free
  • Gamma and EtO sterilization resistant
  • Tough and resilient

Biocompatibility of VESTAMID® Care ME

Biocompatiblity was tested following ISO10993-1 recommendations for a surface medical device with up to 30 days body contact.
 
The material fulfills the requirements of USP<88> class VI.
 
Tests were performed by independent, certified laboratories.

Biocompatibility tests for VESTAMID® Care:
Standard Description
ASTM F756-08 Hemocompatibility
ISO 10993-5 Cytotoxicity
ISO 10993-10 Sensitization: Maximization test according to Magnusson and Kligman
ISO 10993-10 Irritation: Intracutaneous Reactivity
ISO 10993-11 Acute Systemic Toxicity
USP Class VI Acute Systemic Toxicity Intracutaneous Reactivity Muscle Implantation


Processing of VESTAMID® Care
For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY
Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 28 / * cm³/10min ISO 1133
Temperatura 240 / * °C -
Carga 2.16 / * kg -
Contracción posterior al moldeo, paralelo 0.3 / * % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.8 / * % ISO 294-4, 2577
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 125 / - MPa ISO 527
Módulo de plastodeformación, 1000h * / 90 MPa ISO 899-1
Resistencia al impacto Charpy, +23°C N / - kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C N / - kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C N / - kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C N / - kJ/m² ISO 179/1eA
Dureza Shore D 47 / * - ISO 7619-1
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 157 / * °C ISO 11357-1/-3
Temp. de transición vítrea, 10°C/min -50 / * °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 45 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 65 / * °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 70 / * °C ISO 306
Coef.de expansión térmica lineal, paralelo 230 / * E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 210 / * E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espesores de probeta 1.6 / * mm -
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 8.5 / - - IEC 62631-2-1
Constante dieléctrica, 1MHz 4.7 / - - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 1200 / - E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 1300 / - E-4 IEC 62631-2-1
Resistividad volumétrica específica 1E9 / - Ohm*m IEC 62631-3-1
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 1 / * % Sim. to ISO 62
Absorción de humedad 0.4 / * % Sim. to ISO 62
Densidad 1020 / - kg/m³ ISO 1183
Condiciones de transformaciónValorUnidadesMétodo de ensayo
ISO Data
Moldeo por inyección, temperatura de la masa 200 °C ISO 294
Moldeo por inyección, temperatura del molde 35 °C ISO 294
Moldeo por inyección, velocidad de inyección 200 mm/s ISO 294
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Características especiales
Alto impacto o modificado al impacto, Estable a la luz, Estable contra el calor, Esterilizable, Esterilización por óxido de etileno (EtO), Gamma irradiation sterilization
Resistencia quimica
Resistencia química general
Certifications
Grado médico, Biocompatibility ISO 10993, USP Class VI
Applicaciones
Médico
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com