Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® L-R2-GF25 BK - PA12-GF25 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® L-R2-GF25 BK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

Glassfiber reinforced (25%), electrically conductive PA12 resin

VESTAMID® L-R2-GF25 BK glass fiber-reinforced, electrically conductive polyamide 12 for injection molding process, especially for molded parts for explosion-protected equipment and systems.

The parts based on PA 12 absorb only small amounts of water and components made of this material therefore show excellent dimensional stability under changing ambient humidity. The resistance values of the finished parts are dependent on the processing conditions.

VESTAMID® L-R2-GF25 BK is supplied as cylindrical granules ready for processing in moisture-proof polyethylene containers.

The use of colorants may change property values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 
 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM

OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 80 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carga 21.6 / * kg -
Contracción posterior al moldeo, paralelo 0.3 / * % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.8 / * % ISO 294-4, 2577
Densidad de fusión 1020 kg/m³ -
Conductibilidad termica de fusión 0.24 W/(m K) -
Calor especifico de la masa 2020 J/(kg K) -
Temperatura de expulsión 180 °C -
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 6800 / - MPa ISO 527
Resistencia al impacto Charpy, +23°C 75 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
Resistencia al impacto Charpy, -30°C 70 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
Resistencia al impacto Charpy c/entalla, +23°C 10 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Resistencia al impacto Charpy c/entalla, -30°C 11 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 178 / * °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 170 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 175 / * °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 170 / * °C ISO 306
Coef.de expansión térmica lineal, paralelo 100 / * E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 80 / * E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espesores de probeta 1.6 / * mm -
Yellow Card disponible sí / * - -
Combustibilidad a espesor h HB / * class IEC 60695-11-10
Espesores de probeta 0.8 / * mm -
Yellow Card disponible sí / * - -
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Resistividad volumétrica específica 21 / - Ohm*m IEC 62631-3-1
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 1.2 / * % Sim. to ISO 62
Absorción de humedad 0.5 / * % Sim. to ISO 62
Densidad 1270 / - kg/m³ ISO 1183
Condiciones de transformaciónValorUnidadesMétodo de ensayo
ISO Data
Moldeo por inyección, temperatura de la masa 250 °C ISO 294
Moldeo por inyección, temperatura del molde 80 °C ISO 294
Moldeo por inyección, velocidad de inyección 200 mm/s ISO 294
Moldeo por inyección, presión de mantenimiento 70 MPa ISO 294
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola, Negro
Características especiales
Conductividad eléctrica aumentada, Estable a la luz, Estable contra el calor
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.