Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9012 T8 - PA12 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9012 T8:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Heat stabilized and light resistant polyamide 12 compound

VESTAMID® LX9012 T8 has been especially developed for the extrusion and co-extrusion of ski upper and decorative films. Decoration on the bottom side of injection molded sports shoe soles is a further application field.

Films made of VESTAMID® LX9012 T8 feature high transparency, good screen and sublimation printing, outstanding scratch resistance, and excellent impact strength at low temperatures. The semi-crystalline compounds based on PA 12 absorb only low quantities of water.

Therefore, molded parts show excellent dimensional stability, constantly high impact strength, low coefficient of friction and good chemical resistance at changing ambient humidity.

VESTAMID® LX9012 T8 is supplied as cylindrical granules, ready for processing in moisture-proof packaging.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 22 / * cm³/10min ISO 1133
Temperatura 220 / * °C -
Carga 10 / * kg -
Contracción posterior al moldeo, paralelo 1.3 / * % ISO 294-4, 2577
Contracción posterior al moldeo, normal 1.3 / * % ISO 294-4, 2577
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 1100 / - MPa ISO 527
Esfuerzo de fluencia 35 / - MPa ISO 527
Alarg. en límite elástico 5 / - % ISO 527
Alarg. nominal a rotura >50 / - % ISO 527
Resistencia al impacto Charpy, +23°C N / - kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C N / - kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 13 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Resistencia al impacto Charpy c/entalla, -30°C 15 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Dureza Shore D 71 / * - ISO 7619-1
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 176 / * °C ISO 11357-1/-3
Temp. de transición vítrea, 10°C/min 39 / * °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 45 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 120 / * °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 130 / * °C ISO 306
Coef.de expansión térmica lineal, paralelo 130 / * E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espesores de probeta 1.6 / * mm -
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 100Hz 3.8 / - - IEC 62631-2-1
Constante dieléctrica, 1MHz 3 / - - IEC 62631-2-1
Factor de pérdidas dieléctricas, 100Hz 530 / - E-4 IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 280 / - E-4 IEC 62631-2-1
Resistividad volumétrica específica 1E12 / - Ohm*m IEC 62631-3-1
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 1.5 / * % Sim. to ISO 62
Absorción de humedad 0.8 / * % Sim. to ISO 62
Densidad 1010 / - kg/m³ ISO 1183
Características
Procesamiento y forma de entrega
Moldeo por inyección, Extrusion del film
Forma de suministro
Sémola
Características especiales
Alto impacto o modificado al impacto, Estable a la luz, Estable contra el calor, Transparente
Características
Resistente a rayado, Grado tribológico
Resistencia quimica
Resistencia química general
Applicaciones
Equipos deportivos
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.