Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® LX9043 NC - PA12 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® LX9043 NC:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Heat-stabilized polyamide 12 molding compound with improved demoldability

VESTAMID® LX9043 NCis a semi-crystalline, low-viscosity molding compound based on PA12, from which various hollow articles can be produced by rotational molding. The polyamide 12 molding compound is especially suitable for industrial and technical applications with requirements for the manufacture of plastic products of different sizes. The semi-crystalline molding compound absorbs only small amounts of water. Components made from it therefore exhibit excellent dimensional stability under varying ambient humidity.

VESTAMID® LX9043 NC is supplied as cylindrical granules, ready for processing, in moisture-proof bags.
In the undamaged original packaging, the product has a shelf life of at least 2 years if stored in dry rooms at temperatures not exceeding 30°C.


Pigmentation may affect values.

The results shown have been generated from a low number of production lots. Therefore, they are preliminary and not yet the result of a statistical evaluation. Therefore they must not be used to establish specifications.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 63 cm³/10min ISO 1133
Temperatura 230 °C -
Carga 5 kg -
Contracción posterior al moldeo, paralelo 0.9 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 1.2 % ISO 294-4, 2577
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 1107 MPa ISO 527
Esfuerzo de fluencia 39 MPa ISO 527
Alarg. en límite elástico 13 % ISO 527
Alarg. nominal a rotura >50 % ISO 527
Resistencia al impacto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C N kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 5 kJ/m² ISO 179/1eA
Type of failure C - -
Resistencia al impacto Charpy c/entalla, -30°C 4 kJ/m² ISO 179/1eA
Type of failure C - -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 178 °C ISO 11357-1/-3
Temp. de transición vítrea, 10°C/min 40 °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 46 °C ISO 75-1/-2
Estabilidad al calor, 8.00 MPa 96 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 133 °C ISO 306
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de agua 1.5 % Sim. to ISO 62
Densidad 1010 kg/m³ ISO 1183
Características
Procesamiento y forma de entrega
Termoconformación, Moldeo rotacional
Forma de suministro
Sémola, Color natural
Aditivos
Desmoldeante
Características especiales
Estable contra el calor
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.