Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® X7166 - PA12 FR(30) - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® X7166:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto

Low viscosity, self-extinguishing polyamide 12 compound, free of halogen and phosphorus

VESTAMID® X7166 NC is a heat stabilized PA 12 compound containing a non-migrating flame retardant, free of halogen and phosphorus. Tested according to UL94, VESTAMID® X7166 complies with the flammability class V-2.
 
Due to the halogen- and phosphorus-free flame retardants, VESTAMID® X7166 is especially suitable for the electronic and cable industry. It can be used for injection molding as well as for wire extrusion coating.
 
VESTAMID® X7166 is supplied as cylindrical granules, ready for processing, in moisture-proof bags.

Due to the flame retardants, the melt temperature should not exceed 260°C. We recommend melt temperatures within a range of 210°C to 230°C.

The use of colorants may affect property values. 

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM

Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 108 / * cm³/10min ISO 1133
Temperatura 250 / * °C -
Carga 2.16 / * kg -
Contracción posterior al moldeo, paralelo 0.7 / * % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.8 / * % ISO 294-4, 2577
Densidad de fusión 860 kg/m³ -
Conductibilidad termica de fusión 0.2 W/(m K) -
Calor especifico de la masa 3000 J/(kg K) -
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 1890 / - MPa ISO 527
Esfuerzo de fluencia 47 / - MPa ISO 527
Alarg. en límite elástico 5.8 / - % ISO 527
Alarg. nominal a rotura 20 / - % ISO 527
Resistencia al impacto Charpy, +23°C 57 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
Resistencia al impacto Charpy, -30°C 80 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
Resistencia al impacto Charpy c/entalla, +23°C 3 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Resistencia al impacto Charpy c/entalla, -30°C 5 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 178 / * °C ISO 11357-1/-3
Temp. de transición vítrea, 10°C/min 41 / * °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 50 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 140 / * °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 150 / * °C ISO 306
Combustibilidad a 1.5mm esp. nom. V-2 / * class IEC 60695-11-10
Espesores de probeta 1.6 / * mm -
Combustibilidad a espesor h V-2 / * class IEC 60695-11-10
Espesores de probeta 0.8 / * mm -
Yellow Card disponible sí / * - -
Combustibilidad según índice de oxigeno 34 / * % ISO 4589-1/-2
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 1MHz 3.6 / - - IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 340 / - E-4 IEC 62631-2-1
Resistividad volumétrica específica 1E12 / - Ohm*m IEC 62631-3-1
Resistencia dieléctrica 28 / - kV/mm IEC 60243-1
Indice comparativo de linea de fuga 600 / - - IEC 60112
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 1.3 / * % Sim. to ISO 62
Absorción de humedad 0.6 / * % Sim. to ISO 62
Densidad 1070 / - kg/m³ ISO 1183
Condiciones de transformaciónValorUnidadesMétodo de ensayo
ISO Data
Moldeo por inyección, temperatura de la masa 220 °C ISO 294
Moldeo por inyección, temperatura del molde 80 °C ISO 294
Moldeo por inyección, velocidad de inyección 200 mm/s ISO 294
Moldeo por inyección, presión de mantenimiento 70 MPa ISO 294
Funciones
Volumen especifico-temperatura (pvT) , VESTAMID® X7166, PA12 FR(30), Evonik
Características
Procesamiento y forma de entrega
Moldeo por inyección, Extrusión de perfiles, Extrusión de cable, Otros tipos de extrusión, Recubrimiento
Forma de suministro
Sémola, Color natural
Características especiales
Resistencia mejorada al fuego, Sin halógeno, Sin fósforo, Estable contra el calor
Applicaciones
Electrica
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.