Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTORAN® 1900 GF20 HE30018 - PPE-GF20 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTORAN® 1900 GF20 HE30018:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestoran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Modified polyphenylene ether (PPE), heat resistant, glass fiber-reinforced, suitable for K K process

VESTORAN® 1900GF20 HE30018 is the registered trademark of Evonik Degussa GmbH for molding compounds containing poly-2,6-dimethyl-1,4-phenylene ether as polymeric constituent (polyphenylene ether, PPE, also referred to as PPO).

As a material of amorphous structure VESTORAN® 1900GF20 HE30018 shows very small mold shrinkage. Therefore molded parts have a very low tendency to warp.

Moldings of VESTORAN® 1900GF20 HE30018 are dimensionally stable and hydrolysis resistant even in hot water, but are more sensitive to organic solvents than semi-crystalline plastics.

VESTORAN® 1900GF20 HE30018 is resistant to aqueous alkalines and acides, certain alcohols, and glycol solutions.

Glass fiber reinforcement of this molding material combines outstanding heat deflection temperature under load with high strength and rigidity.

VESTORAN®1900GF20 HE30018 is particularly suitable for the adhesion promoter-free manufacturing of plastic/rubber composites patented K&K process ("direct-bonding to rubber").
 
VESTORAN® 1900GF20 HE30018 is supplied as cylindrical granules in polyethylene packaging.
 
Pigmentation may affect values.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 45 cm³/10min ISO 1133
Temperatura 300 °C -
Carga 21.6 kg -
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 5700 MPa ISO 527
Resistencia a la tracción 103 MPa ISO 527
Alargamiento a rotura 2 % ISO 527
Resistencia al impacto Charpy, +23°C 45 kJ/m² ISO 179/1eU
Type of failure C - -
Resistencia al impacto Charpy c/entalla, +23°C 9 kJ/m² ISO 179/1eA
Type of failure C - -
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 190 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 195 °C ISO 75-1/-2
Temp. reblandecimiento Vicat, B 195 °C ISO 306
Coef.de expansión térmica lineal, paralelo 40 E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 50 E-6/K ISO 11359-1/-2
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1200 kg/m³ ISO 1183
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Características especiales
Estable contra el calor
Características
Amorfo, Buenas propiedades de adhesión, Baja deformación
Resistencia quimica
Resistencia al ácido, Resistencia alcalinica, Estabilidad hidrolitica
Disponibilidad regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com