Caracteristicas de procesamiento y fisicas | Valor | Unidades | Método de ensayo |
ASTM Data |
Índice de fluidez, MFI |
3.7 |
g/10min |
ASTM D 1238 |
Temperatura |
190 |
°C |
- |
Carga |
2.16 |
kg |
- |
Propiedades térmicas | Valor | Unidades | Método de ensayo |
Other Standards[S] |
Temperatura de fusión |
106 |
°C |
ExxonMobil Method |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propiedades opticas | Valor | Unidades | Método de ensayo |
ASTM Data |
Brillo |
89 |
- |
ASTM D 2457 |
Other Standards[S] |
Opacidad |
0.4 |
% |
ExxonMobil Method |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Otras propiedades | Valor | Unidades | Método de ensayo |
Other Standards[S] |
Densidad |
889 |
kg/m³ |
ExxonMobil Method |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propiedades mecánicas (Film) | Valor | Unidades | Método de ensayo |
ASTM Data |
Tipo de extrusión |
colada |
- |
- |
Espesor de la muestra |
0.0254 |
mm |
- |
Other Standards[S] |
Esfuerzo de fluencia a tracción, long. |
15.2 |
MPa |
ExxonMobil Method |
Esfuerzo de fluencia a tracción, normal |
13.1 |
MPa |
ExxonMobil Method |
Esfuerzo de fractura a tracción, long. |
62.7 |
MPa |
ExxonMobil Method |
Esfuerzo de fractura a tracción, normal |
35.9 |
MPa |
ExxonMobil Method |
Alargamiento a la rotura, long. |
440 |
% |
ExxonMobil Method |
Alargamiento a la rotura, normal |
790 |
% |
ExxonMobil Method |
S: | These properties are reported by the producer according standards that are different to our defaults. |
Características
Procesamiento y forma de entrega
Extrusion del film
Características
Copolímero
Certifications
RoHS
Applicaciones
Empacado
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com