Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vydyne® R530H BK0201 - PA66-GF30 - Ascend

Material Data Center offers the following functions for Vydyne® R530H BK0201:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vydyne datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Vydyne R530H BK0201 is general purpose, 30% glass-filled, heat-stabilized, high viscosity PA66 based resin designed for injection molding applications. R530H BK0201 offers standard flow with a black surface finish and maintains the excellent resistance typical of PA66 in chemicals, machine and motor oils, solvents, and gasoline.
Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Contracción posterior al moldeo, paralelo 0.4 / * % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.9 / * % ISO 294-4, 2577
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 11000 / 7900 MPa ISO 527
Resistencia a la tracción 200 / 136 MPa ISO 527
Alargamiento a rotura 3.1 / 4 % ISO 527
Módulo de flexión, 23°C 9600 / 6800 MPa ISO 178
Resistencia a la flexión 270 / 170 MPa ISO 178
Resistencia al impacto Charpy, +23°C 76 / 100 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C 66 / 71 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 11 / 14 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 10 / 9.8 kJ/m² ISO 179/1eA
Resistencia al impacto Izod con entalla, +23°C 11 / 13 kJ/m² ISO 180/1A
Resistencia al impacto Izod con entalla 10 / 11 kJ/m² ISO 180/1A
Temperatura -30 °C -
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 262 / * °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 248 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 260 / * °C ISO 75-1/-2
Coef.de expansión térmica lineal, paralelo 19 / * E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 81 / * E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espesores de probeta 1.5 / * mm -
Combustibilidad a espesor h HB / * class IEC 60695-11-10
Espesores de probeta 0.8 / * mm -
Glow Wire Flammability Index (GWFI) 675 °C IEC 60695-2-12
GWFI - thickness tested (1) 0.75 mm -
Glow Wire Flammability Index (GWFI) 675 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.5 mm -
Glow Wire Flammability Index (GWFI) 675 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 700 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.75 mm -
Glow Wire Ignition Temperature (GWIT) 700 °C IEC 60695-2-13
GWIT - thickness tested (2) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 700 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
Combustibilidad UL 94 HB - UL 94
Espesores de probeta 0.75 mm -
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Resistividad volumétrica específica 1E11 / - Ohm*m IEC 62631-3-1
Resistencia dieléctrica 40 / 28 kV/mm IEC 60243-1
Indice comparativo de linea de fuga 325 / - - IEC 60112
ASTM Data
Resistencia al arco 90 / - s ASTM D 495
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 1.3 / * % Sim. to ISO 62
Absorción de humedad 1.9 / * % Sim. to ISO 62
Densidad 1380 / - kg/m³ ISO 1183
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 80 °C -
Tiempo de pre-secado 4 h -
Temperatura de la masa 285 - 305 °C -
Temperatura del molde 65 - 95 °C -
Zona 1 280 - 310 °C -
Zona 2 280 - 310 °C -
Zona 3 280 - 310 °C -
Temperatura de boquilla 280 - 310 °C -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola, Negro
Aditivos
Lubricante
Características especiales
Estable contra el calor
Características
Resistencia a la fatiga
Resistencia quimica
Resistencia química general, Resistencia a solventes, Estabilidad hidrolitica, Resistencia al aceite
Applicaciones
Automotriz, Uso general
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.