Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of XAREC® EA 522 - (PS-SY)-GF22 - Idemitsu Chemicals

Material Data Center offers the following functions for XAREC® EA 522:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Xarec datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
Other Standards[S]
Contracción posterior al moldeo, paralelo 0.3 % Producer Method
Contracción posterior al moldeo, normal 0.6 % Producer Method
S: These properties are reported by the producer according standards that are different to our defaults.
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 8000 MPa ISO 527
Resistencia a la tracción 100 MPa ISO 527
Alargamiento a rotura 2.3 % ISO 527
Módulo de flexión, 23°C 7500 MPa ISO 178
Resistencia a la flexión 155 MPa ISO 178
Resistencia al impacto Charpy, +23°C 39 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 12 kJ/m² ISO 179/1eA
Resistencia al impacto Izod, +23°C 34 kJ/m² ISO 180/1U
Resistencia al impacto Izod con entalla, +23°C 11 kJ/m² ISO 180/1A
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 230 °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 265 °C ISO 75-1/-2
Coef.de expansión térmica lineal, paralelo 24 E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 53 E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. V-0 class IEC 60695-11-10
Espesores de probeta 1.5 mm -
Yellow Card disponible - -
Combustibilidad 5V a espesor h 5VA class IEC 60695-11-20
Espesores de probeta 2.2 mm -
Yellow Card disponible - -
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Indice comparativo de linea de fuga 500 - IEC 60112
ASTM Data
Resistencia dieléctrica, tiempo corto 35 kV/mm ASTM D 149
Resistencia al arco 150 s ASTM D 495
Other Standards[S]
Constante dieléctrica, 1MHz 3 - IEC 60250
Factor de pérdidas dieléctricas, 1MHz 10 E-4 IEC 60250
Resistividad volumétrica específica 1E14 Ohm*m IEC 60093
S: These properties are reported by the producer according standards that are different to our defaults.
Otras propiedadesValorUnidadesMétodo de ensayo
Absorción de humedad 0.01 % Sim. to ISO 62
Densidad 1320 kg/m³ ISO 1183
Recomendación para procesamiento Moldeo por inyecciónValorUnidadesMétodo de ensayo
Temperatura de pre-secado 120 °C -
Tiempo de pre-secado 3 - 5 h -
Temperatura de la masa 280 - 310 °C -
Temperatura del molde 130 - 155 °C -
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola
Características especiales
Resistencia mejorada al fuego, Alto impacto o modificado al impacto
Applicaciones
Electrica
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.