Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Xtel® XE5030NA - PPS-GF - Chevron Phillips Chemical Co. LP

Material Data Center offers the following functions for Xtel® XE5030NA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Xtel datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasValorUnidadesMétodo de ensayo
ISO Data
Contracción posterior al moldeo, paralelo 0.2 % ISO 294-4, 2577
Contracción posterior al moldeo, normal 0.5 % ISO 294-4, 2577
Conductibilidad termica de fusión 0.18 W/(m K) -
ASTM Data
Contracción posterior al moldeo, paralelo 0.002 mm/mm ASTM D 955
Contracción posterior al moldeo, normal 0.005 mm/mm ASTM D 955
Propiedades mecánicasValorUnidadesMétodo de ensayo
ISO Data
Esfuerzo de tracción 145 MPa ISO 527
Módulo de flexión, 23°C 9000 MPa ISO 178
Resistencia al impacto Izod, +23°C 45 kJ/m² ISO 180/1U
Resistencia al impacto Izod con entalla, +23°C 10 kJ/m² ISO 180/1A
ASTM Data
Esfuerzo de tracción 124 MPa ASTM D 638
Resistencia de compresión 207 MPa ASTM D 695
Módulo de flexión 8963 MPa ASTM D 790
Resistencia a la flexión 207 MPa ASTM D 790
Resistencia al impacto Izod con entalla, 1/8 in 112 J/m ASTM D 256
Resistencia al impacto Izod, 1/8 in 854 J/m ASTM D 256
Propiedades térmicasValorUnidadesMétodo de ensayo
ISO Data
Estabilidad al calor, 1.80 MPa 250 °C ISO 75-1/-2
Coef.de expansión térmica lineal, paralelo 20 E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 60 E-6/K ISO 11359-1/-2
Combustibilidad a espesor h V-0 class IEC 60695-11-10
Espesores de probeta 3.0 mm -
ASTM Data
Combustibilidad UL 94 V-0 - UL 94
Espesores de probeta 3.05 mm -
Estabilidad al calor @ 264 psi 252 °C ASTM D 648
Propiedades eléctricasValorUnidadesMétodo de ensayo
ISO Data
Indice comparativo de linea de fuga 100 - IEC 60112
ASTM Data
Resistencia dieléctrica, tiempo corto 19.7 kV/mm ASTM D 149
Factor de pérdidas dieléctricas, 1 MHz 0.009 - ASTM D 150
Constante dieléctrica, 1 MHz 3.6 - ASTM D 150
Resistividad volumétrica 1E15 Ohm*cm ASTM D 257
Resistencia al arco 120 s ASTM D 495
Otras propiedadesValorUnidadesMétodo de ensayo
Densidad 1510 kg/m³ ISO 1183
Absorción de agua, 24hr 0.05 % ASTM D 570
Densidad 1510 kg/m³ ASTM D 792
Características
Forma de suministro
Sémola, Color natural
Características especiales
Alto impacto o modificado al impacto, Estable contra el calor
Características
Bajo olor
Disponibilidad regional
Norteamérica, Europa, Asia Pacifico, América del Sur y Centroaméric, Próximo Oriente/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.