Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Adflex Q 100 F - TPO - LyondellBasell Industries

Material Data Center offers the following functions for Adflex Q 100 F:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Adflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité, MFI 0.6 g/10min ISO 1133
Température 230 °C -
Charge 2.16 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Contrainte à la rupture 10 MPa ISO 527
Déformation à la rupture >50 % ISO 527
Module de flexion, 23°C 100 MPa ISO 178
Résistance au choc Izod avec entaille, +23°C N kJ/m² ISO 180/1A
Résistance au choc Izod avec entaille N kJ/m² ISO 180/1A
Température -20 °C -
Dureté Shore D 30 - ISO 7619-1
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 140 °C ISO 11357-1/-3
Température de fléchissement s/chrg, 0.45 MPa 40 °C ISO 75-1/-2
Température de ramolliss. Vicat, A 60 °C ISO 306
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Brillant 9 - ASTM D 2457
Haze 50 % ASTM D 1003
Propriétés diversesValeurUnitéNorme du test
Masse volumique 880 kg/m³ ISO 1183
Propriétés mécaniques (Grades film)ValeurUnitéNorme du test
ISO Data
Module en traction, parallèle 90 MPa ISO 527-3
Module en traction, perpend. 90 MPa ISO 527-3
Contrainte au seuil, parallèle 7.5 MPa ISO 527-3
Contrainte au seuil, normal 7.5 MPa ISO 527-3
Déformation au seuil, parallèle 40 % ISO 527-3
Déformation au seuil, perpend. 40 % ISO 527-3
Contrainte à la rupture, parallèle 40 MPa ISO 527-3
Contrainte à la rupture, perpend. 37 MPa ISO 527-3
Déformation maximale, parallèle 1000 % ISO 527-3
Déformation maximale, perpend. 1000 % ISO 527-3
Type d'extrusion soufflage - -
Epaisseur des eprouvettes 0.05 mm -
Caractéristiques
Transformation
Extrusion a film soufflé, Extrusion de plaques, Soufflage
Propriétés spéciales
Modifié choc
Caractéristiques
Soft Feel
Certifications
Contact alimentaire, Approuvé pour le contact alimentaire suivant 1935/2004/CE, Approuvé pour le contact alimentaire suivant 10/2011, FDA 21 CFR approbation
Applications
Emballage
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.