Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Apec® 2045 - PC - Covestro Deutschland AG

Material Data Center offers the following functions for Apec® 2045:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Apec datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 8 cm³/10min ISO 1133
Température 330 °C -
Charge 2.16 kg -
Indice de fluidité, MFI 8 g/10min ISO 1133
Température 330 °C -
Charge 2.16 kg -
Retrait au moulage, parallèle 1.1 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.1 % ISO 294-4, 2577
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2400 MPa ISO 527
Contrainte d'écoulement 75 MPa ISO 527
Déformation au seuil d'écoulement 6.8 % ISO 527
Déformation nominale à la rupture >50 % ISO 527
Module de flexion, 23°C 2450 MPa ISO 178
Résistance à la flexion 110 MPa ISO 178
Résistance au choc Charpy, +23°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N kJ/m² ISO 179/1eU
Perforation - force maximum, +23°C 5000 N ISO 6603-2
Perforation - force maximum, -30°C 5500 N ISO 6603-2
Perforation - Energie, +23°C 50 J ISO 6603-2
Perforation - Energie, -30°C 58 J ISO 6603-2
Ball indentation hardness 130 MPa ISO 2039-1
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 173 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 192 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 203 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 65 E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 65 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 mm -
Inflammabilité pr. épaisseur h HB class IEC 60695-11-10
Epaisseur de l'éprouvette 3.0 mm -
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 2.9 - IEC 62631-2-1
Permittivité relative, 1MHz 2.8 - IEC 62631-2-1
Facteur de pertes, 100Hz 10 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 90 E-4 IEC 62631-2-1
Résistivité transversale 1E15 Ohm*m IEC 62631-3-1
Résistivité superficielle 1E16 Ohm IEC 62631-3-2
Rigidité diélectrique 35 kV/mm IEC 60243-1
Propriétés optiquesValeurUnitéNorme du test
ISO Data
Transmittance 90[1] % ISO 13468-1, -2
Other Standards[S]
Indice de réfraction 1.57 - ISO 489
1: 1 mm  S: These properties are reported by the producer according standards that are different to our defaults.
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.3 % Sim. to ISO 62
Absorption d'humidité 0.12 % Sim. to ISO 62
Masse volumique 1130 kg/m³ ISO 1183
Préparation et conditionnement des éprouvettesValeurUnitéNorme du test
ISO Data
Injection, température de la matière fondue 330 °C ISO 294
Injection, température du moule 100 °C ISO 294
injection, vitesse d'injection 200 mm/s ISO 294
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 130 °C -
Pré-séchage - temps 2 - 3 h -
L'humidité de traitement ≤0.02 % -
Température de la matière fondue 330 - 340 °C -
Température du moule 130 - 150 °C -
Zone 1 295 - 305 °C -
Zone 2 305 - 315 °C -
Zone 3 315 - 325 °C -
Température de la buse 325 - 335 °C -
Contre-pression 5 - 15 MPa -
Caractéristiques
Transformation
Moulage par injection
Additifs
Agent de démoulage
Propriétés spéciales
Stabilisé à la chaleur, Stérilisable, Stérilisation à la vapeur
Certifications
Grade médical, Biocompatibility ISO 10993, USP Class VI approbation
Applications
Médical
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.