Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Apec® 1745 RE - PC - Covestro Deutschland AG

Material Data Center offers the following functions for Apec® 1745 RE:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Apec datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
  • MVR (330°C/2.16kg) 17 cm³/10 min
  • easy release
  • for superheated steam sterilization up to 143 °C
  • meets criteria of US Pharmacopeia (USP) Class VI
  • biocompatible according to many ISO 10993-1 test requirements
  • softening temperature (VST/B 120)=170 °C
  • Films for medical packaging
  • Contact lens holders
  • Medical vessels
  • Safety valve for respiration aids
  • Syringe tops
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 17 cm³/10min ISO 1133
Température 330 °C -
Charge 2.16 kg -
Indice de fluidité, MFI 17 g/10min ISO 1133
Température 330 °C -
Charge 2.16 kg -
Retrait au moulage, parallèle 0.8 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.8 % ISO 294-4, 2577
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2400 MPa ISO 527
Contrainte d'écoulement 70 MPa ISO 527
Déformation au seuil d'écoulement 6.8 % ISO 527
Déformation nominale à la rupture >50 % ISO 527
Module de flexion, 23°C 2400 MPa ISO 178
Résistance au choc Charpy, +23°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N kJ/m² ISO 179/1eU
Ball indentation hardness 120 MPa ISO 2039-1
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 148 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 161 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 170 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 65 E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 65 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 mm -
Yellow Card disponible oui - -
Aptitude à l'allumage 25 % ISO 4589-1/-2
Glow Wire Flammability Index (GWFI) 850 °C IEC 60695-2-12
GWFI - thickness tested (1) 2 mm -
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 3 - IEC 62631-2-1
Permittivité relative, 1MHz 2.9 - IEC 62631-2-1
Facteur de pertes, 100Hz 10 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 80 E-4 IEC 62631-2-1
Résistivité transversale >1E13 Ohm*m IEC 62631-3-1
Résistivité superficielle >1E15 Ohm IEC 62631-3-2
Rigidité diélectrique 35 kV/mm IEC 60243-1
Indice de résistance au cheminement 250 - IEC 60112
Propriétés optiquesValeurUnitéNorme du test
ISO Data
Transmittance 88[1] % ISO 13468-1, -2
Other Standards[S]
Indice de réfraction 1.58 - ISO 489
1: Clear transparent materials  S: These properties are reported by the producer according standards that are different to our defaults.
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.3 % Sim. to ISO 62
Absorption d'humidité 0.12 % Sim. to ISO 62
Masse volumique 1170 kg/m³ ISO 1183
Préparation et conditionnement des éprouvettesValeurUnitéNorme du test
ISO Data
Injection, température de la matière fondue 330 °C ISO 294
Injection, température du moule 100 °C ISO 294
Injection, vitesse d'injection 200 mm/s ISO 294
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 130 °C -
Pré-séchage - temps 2 - 3 h -
L'humidité de traitement ≤0.02 % -
Température de la matière fondue 320 - 340 °C -
Température du moule 110 - 130 °C -
Zone 1 290 - 300 °C -
Zone 2 300 - 310 °C -
Zone 3 310 - 320 °C -
Température de la buse 320 - 330 °C -
Contre-pression 5 - 15 MPa -
Caractéristiques
Transformation
Moulage par injection
Additifs
Agent de démoulage
Propriétés spéciales
Stabilisé à la chaleur, Transparent, Stérilisable, Stérilisation à la vapeur
Certifications
Contient des ressources renouvelables, Grade médical, Biocompatibility ISO 10993, USP Class VI approbation, ISCC Plus
Applications
Médical, Emballage
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.