Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of AVALON® 80 ABX - TPU - Huntsman Polymers Corp.

Material Data Center offers the following functions for AVALON® 80 ABX:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Avalon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propriétés mécaniquesValeurUnitéNorme du test
Other Standards[S]
Résistance à la traction 25 MPa DIN 53504
Déformation à la rupture 650 % DIN 53504
Résistance à la déchirure 35 kN/m DIN 53507
Résistance à l'abrasion 55 mm³ DIN 53516
Dureté Shore A 81 - DIN 53505
Dureté Shore D 30 - DIN 53505
S: These properties are reported by the producer according standards that are different to our defaults.
Propriétés diversesValeurUnitéNorme du test
Other Standards[S]
Masse volumique 1150 kg/m³ DIN 53479
S: These properties are reported by the producer according standards that are different to our defaults.
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 80 - 90 °C -
Pré-séchage - temps 2 h -
Température du moule 25 - 50 °C -
Température - Zone d'alimentation 25 - 35 °C -
Zone 1 170 - 190 °C -
Zone 2 175 - 195 °C -
Zone 3 175 - 200 °C -
Température de la buse 170 - 195 °C -
Vitesse de rotation de vis 20 - 80 rpm -
Pressions d'injection 2 - 10 MPa -
Contre-pression 0.03 - 0.3 MPa -
Pression de maintien 1 - 5 MPa -
Caractéristiques
Transformation
Moulage par injection
Caractéristiques
Antidérapant, Résistant aux rayures
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.