Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of BMC 300 - UP-GC26 - LyondellBasell Industries

Material Data Center offers the following functions for BMC 300:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other BMC datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Retrait au moulage , parallèle 0.002 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Module de traction d’élasticité 41.4 MPa ASTM D 638
Résistance de traction à la rupture 41.4 MPa ASTM D 638
Résistance de compression 159 MPa ASTM D 695
Module de flexion 13100 MPa ASTM D 790
Résistance à la flexion 131 MPa ASTM D 790
Dureté A Shore 77 - ASTM D 2240
Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
coefficient de dilatation thermique, long. 162 E-6/K ASTM D 696
Propriétés diversesValeurUnitéNorme du test
Absorption d’eau, 24hr 0.12 % ASTM D 570
Densité 1900 kg/m³ ASTM D 792
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Moulage en vrac
Disponibilité régionale
Amérique du nord
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.