Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Badaflex® TPE-S 40D 1038 - SEBS - Bada AG

Material Data Center offers the following functions for Badaflex® TPE-S 40D 1038:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Badaflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Déformation rémanente en compression à 70 °C, 24h 41 % ISO 815
Déformation rémanente en compression à 100 °C, 24h 70 % ISO 815
Résistance à la déchirure 32 kN/m ISO 34-1
Dureté Shore D 40 - ISO 7619-1
Other Standards[S]
Résistance à la traction 12 MPa DIN 53504
Déformation à la rupture TPE 500 % DIN 53504
S: These properties are reported by the producer according standards that are different to our defaults.
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1180 kg/m³ ISO 1183
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 60 - 70 °C -
Pré-séchage - temps 2 - 3 h -
L'humidité de traitement ≤0.1 % -
Température de la matière fondue 190 - 220 °C -
Température du moule 20 - 40 °C -
Caractéristiques
Transformation
Moulage par injection
Caractéristiques
Bonne adhérence
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.