Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CP PRYME® Polycarbonate PC100RUL-18M Clear - PC - Chase Plastics

Material Data Center offers the following functions for CP PRYME® Polycarbonate PC100RUL-18M Clear:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other CP Pryme datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Indice de fluidité, MFI 18 g/10min ASTM D 1238
Température 300 °C -
Charge 1.2 kg -
Retrait au moulage , parallèle 0.006 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Résistance au choc Charpy, +23°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 65 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 12 kJ/m² ISO 179/1eA
Résistance au choc Izod, +23°C N kJ/m² ISO 180/1U
Résistance au choc Izod avec entaille, +23°C 65 kJ/m² ISO 180/1A
Résistance au choc Izod avec entaille 11 kJ/m² ISO 180/1A
Température -30 °C -
ASTM Data
Module de traction d’élasticité 62.1 MPa ASTM D 638
Résistance de traction à la rupture 68.9 MPa ASTM D 638
Allongement d’élasticité 7 % ASTM D 638
Allongement à la rupture 130 % ASTM D 638
Module de flexion 2340 MPa ASTM D 790
Dureté Rockwell R118 - ASTM D 785
Taber abrasion résistance 10 mg/1000 cycles ASTM D 1044
Izod choc avec entaille, 1/8 in 690 J/m ASTM D 256
Résistance au choc Izod, 1/8 in 3200 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
UL 94 inflammabilité HB - UL 94
DTUL à 66 psi 138 °C ASTM D 648
DTUL à 264 psi 129 °C ASTM D 648
Vicat température 154 °C ASTM D 1525
Conductivité thermique, l'état solide 0.036 W/(m K) ASTM C 177
Chaleur spécifique 1260 J/(kg K) ASTM C 351
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Haze 1 % ASTM D 1003
Lumière á Transmittance 88 % ASTM D 1003
Indice de réfraction 1.59 - ASTM D 542
Propriétés diversesValeurUnitéNorme du test
Absorption d’eau, 24hr 0.15 % ASTM D 570
Absorption d’eau, équilibre 0.35 % ASTM D 570
Densité 1200 kg/m³ ASTM D 792
Caractéristiques
Conditionnement
Granulés
Propriétés spéciales
Transparent
Disponibilité régionale
Amérique du nord
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com