Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of Cadence™ GS5 - Copolyester - Eastman Chemical Co.
unit conversion, PDF datasheet print, comparison with other plastics
Check here, which other Cadence datasheets, application examples or technical articles are available in Material Data Center
Eastman Cadence™ GS5 is an amorphous copolyester with improved processability for film calendering.
Calendered films made of Eastman Cadence™ copolyester are non-crystallizing, are halogen-free, offer wide calendering and thermoforming windows and have good low-temperature toughness. They are cooperative in secondary operations such as solvent-bonding, lamination, decoration, cold-forming, punching/cutting and mbossment.
Eastman Cadence™ resins require no pre-drying or additional stabilizers.
Propriétés mécaniques | Valeur | Unité | Norme du test | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ASTM Data | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Dureté A Shore | 83 | - | ASTM D 2240 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Dureté D Shore | 73 | - | ASTM D 2240 |
Propriétés diverses | Valeur | Unité | Norme du test |
Densité | 1270 | kg/m³ | ASTM D 792 |
Propriétés mécaniques (Grades film) | Valeur | Unité | Norme du test | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ASTM Data | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Module en traction, long. | 1870 | MPa | ASTM D 882 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Module en traction, trav. | 1820 | MPa | ASTM D 882 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Résistance de traction à la rupture, long. | 50 | MPa | ASTM D 882 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Résistance de traction à la rupture, trav. | 48 | MPa | ASTM D 882 |