Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CELSTRAN® PA66-GF40-02P11/15 - PA66-GLF40 - Celanese

Material Data Center offers the following functions for CELSTRAN® PA66-GF40-02P11/15:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Celstran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 13700 / 10000 MPa ISO 527
Contrainte à la rupture 190 / 160 MPa ISO 527
Déformation à la rupture 1.6 / 2 % ISO 527
Résistance au choc Charpy, +23°C 40 / 45 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 41 / - kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 23 / 18 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 23 / - kJ/m² ISO 179/1eA
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 261 / * °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 255 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 8.00 MPa 240 / * °C ISO 75-1/-2
Propriétés diversessec / condUnitéNorme du test
Masse volumique - / 1460 kg/m³ ISO 1183
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 80 °C -
Pré-séchage - temps 4 h -
Température de la matière fondue 300 - 315 °C -
Température du moule 90 - 120 °C -
Fonctions
Contrainte / Déformation , CELSTRAN® PA66-GF40-02P11/15 (sec), PA66-GLF40, Celanese
Contrainte / Déformation , CELSTRAN® PA66-GF40-02P11/15 (cond.), PA66-GLF40, Celanese
Module sécant / Déformation , CELSTRAN® PA66-GF40-02P11/15 (sec), PA66-GLF40, Celanese
Module sécant / Déformation , CELSTRAN® PA66-GF40-02P11/15 (cond.), PA66-GLF40, Celanese
Caractéristiques
Transformation
Moulage par injection, Extrusion de profilés, Extrusion de plaques, Extrusion (autres), Soufflage, Moulage par transfert
Conditionnement
Granulés
Additifs
Lubrifiant
Propriétés spéciales
Stabilisé à la chaleur
Caractéristiques
Long fiber reinforced
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific
Autres informations
Moulages par injection
It is recommended to dry in a dehumidifying dryer: 4 hours at 80 °C.

During the processing of CELSTRAN it is important to watch and
control melt shear, for excessive shear reduces fiber length and
mechanical performance as well.

Processing recommendation:

- Conventional 3 zone screw, screw diameter minimum 40 mm
- Design flow channels for low melt shear
- Back pressure and screw rotation to realize a continous
plastification performance and thus a homogeneous melt.
- Apply higher temperature settings than for short fiber compounds

Melt temperature (in the screw anteroom) 300-315 °C
Mold surface temperature 90-120 °C
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.