Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Clearflex® CL 508 - (PE-MD) - Versalis S.p.A

Material Data Center offers the following functions for Clearflex® CL 508:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Clearflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité, MFI 2.7 g/10min ISO 1133
Température 190 °C -
Charge 2.16 kg -
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 128 °C ISO 11357-1/-3
Coeffic. de dilatation therm. linéique, parallèle 35 E-6/K ISO 11359-1/-2
Propriétés optiquesValeurUnitéNorme du test
ISO Data
Brillance, 45° 84 - ISO 2813
Haze 3.5 - ISO 14782
Propriétés diversesValeurUnitéNorme du test
Masse volumique 935 kg/m³ ISO 1183
Propriétés mécaniques (Grades film)ValeurUnitéNorme du test
ISO Data
Contrainte au seuil, parallèle 16 MPa ISO 527-3
Contrainte au seuil, normal 17 MPa ISO 527-3
Contrainte à la rupture, perpend. 30 MPa ISO 527-3
Déformation maximale, parallèle 660 % ISO 527-3
Déformation maximale, perpend. 800 % ISO 527-3
Coefficient de friction dynamique 0.5 - ISO 8295
Type d'extrusion cast - -
Epaisseur des eprouvettes 0.023 mm -
Caractéristiques
Transformation
Extrusion de films
Conditionnement
Granulés
Caractéristiques
Copolymère, Octène copolymère
Résistance Chimique
Résistance à oxydation
Disponibilité régionale
Europe, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.