Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Cristal™ Renew 400-100 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Cristal™ Renew 400-100:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Cristal datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Eastman Cristal™ 400-100 Renew copolyester is a high flow product. It is designed and engineered specifically for

cosmetics packaging applications. With its unsurpassed color and clarity and an unmatched ability to mold thick

parts with improved gate aesthetics, Cristal™ 400-100 Renew is clearly a well suited copolyester for premium

cosmetics packaging. Other outstanding features are excellent chemical resistance, high gloss, and improvements

in processing such as faster cycle times, and lower scrap rates. Cristal™ 400-100 Renew is also ideally suited for

two-shot molding techniques due to its lower processing temperatures, very slow crystallization rate, and flow

characteristics.

Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a

global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are

produced with ISCC certified circular content by mass balance allocation.


Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Retrait au moulage , parallèle 0.0035 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2000 MPa ISO 527
Contrainte d'écoulement 49 MPa ISO 527
Déformation au seuil d'écoulement 4.2 % ISO 527
Contrainte à la rupture 21 MPa ISO 527
Déformation à la rupture 36 % ISO 527
ASTM Data
Module en traction 2030 MPa ASTM D 638
Module de traction d’élasticité 50 MPa ASTM D 638
Résistance de traction à la rupture 25 MPa ASTM D 638
Allongement d’élasticité 4.4 % ASTM D 638
Allongement à la rupture 38 % ASTM D 638
Module de flexion 1810 MPa ASTM D 790
Résistance à la flexion 66 MPa ASTM D 790
Dureté Rockwell R 102 - ASTM D 785
Izod choc avec entaille, 1/8 in 104 J/m ASTM D 256
Izod choc avec entaille, bas température 38 J/m ASTM D 256
Température -40 °C -
Résistance au choc Izod, 1/8 in N J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
DTUL à 66 psi 68 °C ASTM D 648
DTUL à 264 psi 61 °C ASTM D 648
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Haze 0.24 % ASTM D 1003
Lumière á Transmittance 91.8 % ASTM D 1003
Propriétés diversesValeurUnitéNorme du test
Densité 1280 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 65 °C -
Pré-séchage - temps 8 h -
Température de la matière fondue 205 - 240 °C -
Température du moule 16 - 38 °C -
Caractéristiques
Transformation
Moulage par injection, Extrusion (autres)
Propriétés spéciales
Modifié choc, Transparent
Caractéristiques
High Gloss, Copolymère
Résistance Chimique
Résistance chimique générale
Certifications
ISCC Plus
Applications
Emballage
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.