Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CYROLITE® G 20 - MBS - Röhm GmbH

Material Data Center offers the following functions for CYROLITE® G 20:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Cyrolite datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Productprofil:

CYROLITE G-20 compound is an impact-modified acrylic-based multipolymer for molding and extrusion of medical applications.

Typical properties of CYROLITE G-20 compound are:


• excellent chemical resistance to fats and oils
• excellent bonding and welding capabilities
• excellent bonding to PVC tubing
• good impact strength
• good light transmission
• good heat resistance
• good resistance to EtO, gamma and E-beam sterilization.

Application:

Used for injection molding and extrusion of medical devices, medical packaging, as well as food packaging, toys and appliance parts.

Example:

Y-sites, luer connectors and check valves.

Processing:

CYROLITE G-20 compound can be processed in injection molding machines and extrusion lines with 3- zone general purpose screws.

Physical Form / Packaging:

Available in 1500 lb. gaylord boxes; other packaging available on request.

Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 1.9 cm³/10min ISO 1133
Température 230 °C -
Charge 3.8 kg -
Densité du fondu 998 kg/m³ -
Conductivité thermique du fondu 0.163 W/(m K) -
Chaleur spécifique du fondu 2260 J/(kg K) -
Diffusivité thermique 7.22E-8 m²/s -
Température d'éjection 75 °C -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2400 MPa ISO 527
Contrainte d'écoulement 51 MPa ISO 527
Déformation au seuil d'écoulement 3.4 % ISO 527
Déformation nominale à la rupture 11 % ISO 527
Résistance au choc Charpy, +23°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 11 kJ/m² ISO 179/1eA
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 79 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 83 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 95 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 90 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 mm -
Aptitude à l'allumage 18 % ISO 4589-1/-2
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Résistivité transversale >1E13 Ohm*m IEC 62631-3-1
Résistivité superficielle 1E13 Ohm IEC 62631-3-2
Propriétés diversesValeurUnitéNorme du test
Absorption d'humidité 0.3 % Sim. to ISO 62
Masse volumique 1110 kg/m³ ISO 1183
Préparation et conditionnement des éprouvettesValeurUnitéNorme du test
ISO Data
Injection, température de la matière fondue 240 °C ISO 294
Injection, température du moule 65 °C ISO 294
Injection, vitesse d'injection 195 mm/s ISO 294
Fonctions
Viscosité / Vitesse de cisaillement , CYROLITE® G 20, MBS, Röhm
Contrainte de cisaillement / Vit. de cisaillement , CYROLITE® G 20, MBS, Röhm
Contrainte / Déformation , CYROLITE® G 20, MBS, Röhm
Module sécant / Déformation , CYROLITE® G 20, MBS, Röhm
Caractéristiques
Transformation
Moulage par injection, Extrusion de films, Extrusion de profilés, Extrusion (autres), Thermoformage
Conditionnement
Granulés
Propriétés spéciales
Modifié choc, Stabilisé à la chaleur, Transparent, Stérilisable, Stérilisation par oxyde d'éthylène (EtO), Stérilisation par rayonnement gamma, Electron beam (e-beam) sterilization
Caractéristiques
Bonne adhérence, Soudable
Résistance Chimique
Résistance aux graisses, Résistance aux huiles
Certifications
Contact alimentaire
Applications
Médical, Emballage
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Autres informations
Moulages par injection
PREPROCESSING
Predrying temperature: 80 °C
Predrying time: 3 - 4 h
PROCESSING
Melt temperature: 205 - 245°C
Mold temperature:50 - 80°C
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.