Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delas 175 - (NBR+PVC) - Lingen Plastic Rubber Co., Ltd.

Material Data Center offers the following functions for Delas 175:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Delas datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Dureté A Shore 75 - ASTM D 2240
Résistance au déchirement 36 kN/m ASTM D 624
Compression rémanente, 22 hr @ 158 °F 66 % ASTM D 395
Module de traction 12 MPa ASTM D 412
Propriétés diversesValeurUnitéNorme du test
Densité 1270 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 60 °C -
Pré-séchage - temps 4 - 6 h -
Température de la matière fondue 170 °C -
Température du moule 30 - 80 °C -
Zone 1 130 - 140 °C -
Zone 2 140 - 160 °C -
Zone 3 160 - 190 °C -
Température de la buse 170 - 190 °C -
Vitesse de rotation de vis 100 - 200 rpm -
Contre-pression 0.05 - 0.5 MPa -
Recommandations pour la transformation ExtrusionValeurUnitéNorme du test
Pré-séchage - température 60 °C -
Pré-séchage - temps 4 - 6 h -
Température de la matière fondue 160 °C -
Température du moule 150 - 170 °C -
Température - Zone d'alimentation 130 - 140 °C -
Zone 1 140 - 150 °C -
Zone 2 140 - 150 °C -
Zone 3 150 - 170 °C -
Caractéristiques
Transformation
Moulage par injection, Extrusion (autres)
Propriétés spéciales
Stabilisé aux intempéries
Résistance Chimique
Résistance aux graisses
Disponibilité régionale
Asia Pacific
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.