Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ MN004 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ MN004:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Eastar™ Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar™ MN004 contains a mold release.




Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Retrait au moulage , parallèle 0.0035 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Contrainte d'écoulement 46 MPa ISO 527
Déformation au seuil d'écoulement 4.4 % ISO 527
Contrainte à la rupture 47 MPa ISO 527
Déformation à la rupture 230 % ISO 527
Module de flexion, 23°C 1800 MPa ISO 178
Résistance au choc Izod avec entaille, +23°C 125 kJ/m² ISO 180/1A
Résistance au choc Izod avec entaille 7.4 kJ/m² ISO 180/1A
Température -40 °C -
Perforation - Energie, +23°C 14 J ISO 6603-2
ASTM Data
Module de traction d’élasticité 45 MPa ASTM D 638
Résistance de traction à la rupture 52 MPa ASTM D 638
Allongement d’élasticité 5 % ASTM D 638
Allongement à la rupture 330 % ASTM D 638
Module de flexion 1800 MPa ASTM D 790
Dureté Rockwell R 105 - ASTM D 785
Izod choc avec entaille, 1/8 in N J/m ASTM D 256
Izod choc avec entaille, bas température 64 J/m ASTM D 256
Température -40 °C -
Résistance au choc Izod, 1/8 in N J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 65 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 74 °C ISO 75-1/-2
Température de ramolliss. Vicat, A 88 °C ISO 306
Température de ramolliss. Vicat, B 79 °C ISO 306
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 mm -
Inflammabilité pr. épaisseur h HB class IEC 60695-11-10
Epaisseur de l'éprouvette 3.2 mm -
ASTM Data
UL 94 inflammabilité HB - UL 94
Épaisseur testée 1.6 mm -
DTUL à 66 psi 74 °C ASTM D 648
DTUL à 264 psi 64 °C ASTM D 648
Vicat température 88 °C ASTM D 1525
Conductivité thermique, l'état solide 0.0274 W/(m K) ASTM C 177
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Haze 1 % ASTM D 1003
Lumière á Transmittance 89 % ASTM D 1003
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1230 kg/m³ ISO 1183
Absorption d’eau, 24hr 0.13 % ASTM D 570
Densité 1230 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 75 °C -
Pré-séchage - temps 6 h -
Température de la matière fondue 250 - 270 °C -
Température du moule 15 - 40 °C -
Caractéristiques
Transformation
Moulage par injection
Additifs
Agent de démoulage
Propriétés spéciales
Modifié choc
Caractéristiques
Copolymère
Résistance Chimique
Résistance chimique générale
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.