Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Eastar™ CN015-75 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Eastar™ CN015-75:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Eastar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit

Eastar™ Renew CN015-75 is a high flow product that contains a mold release to provide ease of demolding.

Designed specifically for the unique requirements of luxury cosmetic packaging, our premier PCTA copolyester delivers unsurpassed color and clarity and a capability to mold thick parts with improved gate aesthetics. Other outstanding features of Eastar™ Renew CN015-75 include excellent chemical resistance, high gloss, and process enhancements such as faster drying times, faster cycle times, and lower scrap rates. Eastar™ Renew CN015-75 is also ideally suited for two-shot molding techniques due to its lower processing temperatures, very slow crystallization rate, and flow characteristics.

Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Renew polymers enable a brand to reduce consumption of fossil feedstock-based plastics, achieve sustainability targets without compromise, and be a fast mover in a growing market for sustainable consumer products.


Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Retrait au moulage , parallèle 0.003 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Module de traction d’élasticité 50 MPa ASTM D 638
Résistance de traction à la rupture 35 MPa ASTM D 638
Allongement d’élasticité 4.5 % ASTM D 638
Allongement à la rupture 193 % ASTM D 638
Module de flexion 1800 MPa ASTM D 790
Résistance à la flexion 67 MPa ASTM D 790
Dureté Rockwell R 105 - ASTM D 785
Izod choc avec entaille, 1/8 in 70 J/m ASTM D 256
Izod choc avec entaille, bas température 38 J/m ASTM D 256
Température -40 °C -
Résistance au choc Izod, 1/8 in N J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
DTUL à 66 psi 71 °C ASTM D 648
DTUL à 264 psi 63 °C ASTM D 648
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Haze 0.6 % ASTM D 1003
Lumière á Transmittance 90 % ASTM D 1003
Propriétés diversesValeurUnitéNorme du test
Densité 1200 kg/m³ ASTM D 792
Recommandations pour la transformation ExtrusionValeurUnitéNorme du test
Pré-séchage - température 60 °C -
Pré-séchage - temps 2 - 4 h -
Température de la matière fondue 225 - 245 °C -
Température du moule 16 - 50 °C -
Caractéristiques
Transformation
Extrusion (autres)
Conditionnement
Couleurs naturelles
Additifs
Agent de démoulage
Propriétés spéciales
Modifié choc, Transparent
Caractéristiques
Soudage à la chaleur, High Gloss, Copolymère
Résistance Chimique
Résistance chimique générale
Certifications
ISCC Plus
Applications
Emballage
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.