Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ECOZEN® HF002 - Copolyester - SK Chemicals

Material Data Center offers the following functions for ECOZEN® HF002:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ecozen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
ECOZEN, conceived and developed by SK Chemicals is a bio-based, heat-resistant, and transparent bio-copolyester.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Retrait au moulage , parallèle 0.0035 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Contrainte d'écoulement 59 MPa ISO 527
Déformation au seuil d'écoulement 4.3 % ISO 527
Contrainte à la rupture 34 MPa ISO 527
Déformation à la rupture 300 % ISO 527
Module de flexion, 23°C 2400 MPa ISO 178
Résistance à la flexion 79 MPa ISO 178
Résistance au choc Izod avec entaille, +23°C 3.7 kJ/m² ISO 180/1A
Dureté Rockwell R 115 - ISO 2039-2
ASTM Data
Module de traction d’élasticité 60 MPa ASTM D 638
Résistance de traction à la rupture 42.2 MPa ASTM D 638
Allongement d’élasticité 5 % ASTM D 638
Allongement à la rupture 220 % ASTM D 638
Module de flexion 2403 MPa ASTM D 790
Résistance à la flexion 86.3 MPa ASTM D 790
Dureté Rockwell R 115 - ASTM D 785
Izod choc avec entaille, 1/8 in 65 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 72 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 83 °C ISO 75-1/-2
ASTM Data
DTUL à 66 psi 79 °C ASTM D 648
DTUL à 264 psi 68 °C ASTM D 648
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Haze 1 % ASTM D 1003
Lumière á Transmittance 86 % ASTM D 1003
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1330 kg/m³ ISO 1183
Densité 1330 kg/m³ ASTM D 792
Caractéristiques
Transformation
Extrusion de films, Extrusion de plaques, Soufflage
Propriétés spéciales
Stabilisé à la chaleur, Transparent
Caractéristiques
Copolymère
Résistance Chimique
Résistance chimique générale
Certifications
Contient des ressources renouvelables, RoHS
Applications
Emballage
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.