Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Exceed™ 1518HA - PE - ExxonMobil Chemical

Material Data Center offers the following functions for Exceed™ 1518HA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Exceed datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Indice de fluidité, MFI 1.5 g/10min ASTM D 1238
Température 190 °C -
Charge 2.16 kg -
Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
Température de fusion 118 °C ASTM D 3418
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Brillant 20 - ASTM D 2457
Haze 40 % ASTM D 1003
Propriétés diversesValeurUnitéNorme du test
Densité 918 kg/m³ ASTM D 792
Propriétés mécaniques (Grades film)ValeurUnitéNorme du test
ASTM Data
Module de traction d’élasticité, long. 8.96 MPa ASTM D 882
Module de traction d’élasticité, trav. 9.65 MPa ASTM D 882
Résistance de traction à la rupture, long. 63.4 MPa ASTM D 882
Résistance de traction à la rupture, trav. 57.9 MPa ASTM D 882
Allongement à la rupture, long. 550 % ASTM D 882
Allongement à la rupture, trav. 690 % ASTM D 882
Type d'extrusion soufflage - -
Epaisseur des eprouvettes 0.0254 mm -
Caractéristiques
Transformation
Extrusion a film soufflé, Extrusion de films
Propriétés spéciales
Modifié choc
Caractéristiques
Propriétés barrière, Bon tirage, Stabilité thermique, Copolymère, Hexène copolymère
Certifications
Contact alimentaire
Applications
Emballage
Disponibilité régionale
Amérique du nord, South and Central America
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.