Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Genestar™ G1300H-F02 - PA9T-GF30 - Kuraray Co., Ltd.

Material Data Center offers the following functions for Genestar™ G1300H-F02:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Genestar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
GENESTAR G1300H-F02 is an injection molding grade with 30% GF developed for reflow applications. It is halogen-free and has a HB flammability.

Thanks to its JEDEC MSL 1 rating (moisture sensitive level 1), this grade shows an excellent resistance to blisters.

GENESTAR G1300H-F02 is suitable for all kind of reflow components such as:
- FPC connectors
- Board-to-board connectors
- wire-to-board connectors
- automotive connectors
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Retrait au moulage, parallèle 0.3 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.0 % ISO 294-4, 2577
ASTM Data
Indice de fluidité, MFI 45 g/10min ASTM D 1238
Température 320 °C -
Charge 2.16 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 9500 MPa ISO 527
Contrainte à la rupture 151 MPa ISO 527
Déformation à la rupture 1.9 % ISO 527
Résistance au choc Charpy (entaillé), +23°C 11 kJ/m² ISO 179/1eA
ASTM Data
Module de traction 160 MPa ASTM D 638
Module de flexion 8500 MPa ASTM D 790
Résistance à la flexion 205 MPa ASTM D 790
Izod choc avec entaille, 1/8 in 105 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 306 °C ISO 11357-1/-3
Température de transition vitreuse, 10°C/min 125 °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 290 °C ISO 75-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
ASTM Data
UL 94 inflammabilité HB - UL 94
DTUL à 264 psi 290 °C ASTM D 648
Température de fusion 306 °C ASTM D 3418
Température de transition vitreuse 125 °C ASTM E 1356
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Rigidité diélectrique 28 kV/mm IEC 60243-1
Indice de résistance au cheminement 600 - IEC 60112
ASTM Data
Rigidité diélectrique, peu de temps 30 kV/mm ASTM D 149
Résistance volumique >1E15 Ohm*cm ASTM D 257
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.18 % Sim. to ISO 62
Masse volumique 1370 kg/m³ ISO 1183
Densité 1370 kg/m³ ASTM D 792
Fonctions
Contrainte / Déformation , Genestar™ G1300H-F02, PA9T-GF30, Kuraray
Module sécant / Déformation , Genestar™ G1300H-F02, PA9T-GF30, Kuraray
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Propriétés spéciales
Ignifugé, Sans halogène, Stabilisé à la chaleur
Caractéristiques
Soudable
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.