Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kurarity™ LA2140 - TPE - Kuraray Co., Ltd.

Material Data Center offers the following functions for Kurarity™ LA2140:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kurarity datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
KURARITY is non-crystalline block copolymer and does not have melting point.
All the KURARITY grades show similar low temperature properties which result from Tg of poly (n-butyl acrylate) or poly (n-butyl acrylate/2-ethylhexyl acrylate) and heat resistance from Tg of PMMA.
LA series : n-butyl acrylate based block copolymers.
Suitable Applications: For PSA, Compound, Additives.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité, MFI 64 g/10min ISO 1133
Température 190 °C -
Charge 2.16 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Résistance au choc Charpy (entaillé), +23°C N kJ/m² ISO 179/1eA
Résistance à la traction 5.5 MPa ISO 37
Dureté Shore A 22 - ISO 7619-1
Dureté Shore D 5 - ISO 7619-1
Other Standards[S]
Contrainte à 100% de déformation 1.5 MPa ISO 37
S: These properties are reported by the producer according standards that are different to our defaults.
Propriétés thermiquesValeurUnitéNorme du test
Other Standards[S]
Conductivité thermique, l'état solide 0.17 W/(m K) ASTM E 1530
S: These properties are reported by the producer according standards that are different to our defaults.
Propriétés optiquesValeurUnitéNorme du test
ISO Data
Haze 4 - ISO 14782
Other Standards[S]
Lumière á Transmittance 92 % ISO 13468-1
S: These properties are reported by the producer according standards that are different to our defaults.
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1080 kg/m³ ISO 1183
Caractéristiques
Conditionnement
Granulés
Propriétés spéciales
Stabilisé aux intempéries, Transparent
Caractéristiques
Mélange de résine, Bonne adhérence, Faible odeur, Copolymère
Résistance Chimique
Résistance aux acides, Résistance aux alcalis , Résistance aux huiles
Applications
Automobile, Électrotechnique et électrique
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.