Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LASULF - PSU - LATI Industria Termoplastici S.p.A.

Material Data Center offers the following functions for LASULF:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lasulf datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Retrait au moulage, parallèle 0.7 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.8 % ISO 294-4, 2577
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2500 MPa ISO 527
Contrainte d'écoulement 70 MPa ISO 527
Déformation au seuil d'écoulement 5.5 % ISO 527
Déformation à la rupture 100 % ISO 527
Résistance au choc Charpy, +23°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 5 kJ/m² ISO 179/1eA
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 165 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 180 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 175 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 48 E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 49 E-6/K ISO 11359-1/-2
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (1) 1 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 2 mm -
ASTM Data
UL 94 inflammabilité HB - UL 94
Épaisseur testée 1.5 mm -
Indice limite d’oxygène 30 % ASTM D 2863
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Indice de résistance au cheminement 150 - IEC 60112
ASTM Data
Rigidité diélectrique, peu de temps 17 kV/mm ASTM D 149
Résistance de la surface 1E12 Ohm ASTM D 257
Propriétés diversesValeurUnitéNorme du test
Masse volumique 1230 kg/m³ ISO 1183
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 120 - 150 °C -
Pré-séchage - temps 3 h -
Température de la matière fondue 300 - 320 °C -
Température du moule 120 - 140 °C -
Caractéristiques
Transformation
Moulage par injection
Caractéristiques
Bas fumée
Disponibilité régionale
Europe
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.