Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEONA™ 1330G - PA66-GF... - Asahi Kasei

Material Data Center offers the following functions for LEONA™ 1330G:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Leona datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction 9800 / 6700 MPa ISO 527
Contrainte à la rupture 144 / 107 MPa ISO 527
Déformation à la rupture 4 / 6 % ISO 527
Module de flexion, 23°C 8700 / 6000 MPa ISO 178
Résistance à la flexion 235 / 165 MPa ISO 178
Résistance au choc Charpy, +23°C 71 / 78 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 10 / 13 kJ/m² ISO 179/1eA
Dureté Rockwell R 120 - ISO 2039-2
ASTM Data
Module de traction 157 / 118 MPa ASTM D 638
Allongement à la rupture 3 / 3 % ASTM D 638
Module de flexion 8000 / 6300 MPa ASTM D 790
Résistance à la flexion 245 / 177 MPa ASTM D 790
Dureté Rockwell M 89 / M 60 - ASTM D 785
Taber abrasion résistance 9 mg/1000 cycles ASTM D 1044
Izod choc avec entaille, 1/8 in 98 / 118 J/m ASTM D 256
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 246 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 261 / * °C ISO 75-1/-2
Inflammabilité pr. épaisseur h HB / * class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 / * mm -
Yellow Card disponible oui / * - -
ASTM Data
UL 94 inflammabilité HB - UL 94
Épaisseur testée 0.75 mm -
coefficient de dilatation thermique, long. 30 E-6/K ASTM D 696
DTUL à 66 psi 260 °C ASTM D 648
DTUL à 264 psi 248 °C ASTM D 648
Propriétés diversessec / condUnitéNorme du test
Absorption d'humidité 1.4 / * % Sim. to ISO 62
Masse volumique 1480 / - kg/m³ ISO 1183
Densité 1480 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 80 - 90 °C -
Pré-séchage - temps 2 - 3 h -
Température de la matière fondue 275 - 295 °C -
Température du moule 75 - 85 °C -
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Additifs
Lubrifiant
Caractéristiques
Grade tribologique
Applications
Automobile
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.