Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luflexen hyPE 36R FA - (PE-LLD) - LyondellBasell Industries

Material Data Center offers the following functions for Luflexen hyPE 36R FA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Luflexen datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité, MFI 2.5 g/10min ISO 1133
Température 190 °C -
Charge 2.16 kg -
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 127 °C ISO 11357-1/-3
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Brillant 115 - ASTM D 2457
Haze 7 % ASTM D 1003
Propriétés diversesValeurUnitéNorme du test
Masse volumique 936 kg/m³ ISO 1183
Propriétés mécaniques (Grades film)ValeurUnitéNorme du test
ISO Data
Déformation maximale, parallèle 750 % ISO 527-3
Déformation maximale, perpend. 850 % ISO 527-3
Type d'extrusion cast - -
Epaisseur des eprouvettes 0.025 mm -
Recommandations pour la transformation ExtrusionValeurUnitéNorme du test
Type of extrusion film - -
Température de la matière fondue 190 - 250 °C -
Caractéristiques
Transformation
Extrusion a film soufflé, Extrusion de films
Conditionnement
Granulés
Propriétés spéciales
Modifié choc
Caractéristiques
Bas gel
Résistance Chimique
Résistance à oxydation
Certifications
Contact alimentaire
Applications
Emballage
Disponibilité régionale
Europe
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.