Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LUPOL ST7540 - TPO - LG Chem

Material Data Center offers the following functions for LUPOL ST7540:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Lupol datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité, MFI 9 g/10min ISO 1133
Température 230 °C -
Charge 2.16 kg -
Retrait au moulage, parallèle 0.6 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.7 % ISO 294-4, 2577
ASTM Data
Indice de fluidité, MFI 9 g/10min ASTM D 1238
Température 230 °C -
Charge 2.16 kg -
Retrait au moulage , parallèle 0.0055 mm/mm ASTM D 955
Retrait au moulage, perpendiculaire 0.007 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Contrainte d'écoulement 9.5 MPa ISO 527
Déformation au seuil d'écoulement 9 % ISO 527
Contrainte à la rupture 11 MPa ISO 527
Déformation à la rupture 500 % ISO 527
Module de flexion, 23°C 510 MPa ISO 178
Résistance à la flexion 13 MPa ISO 178
Résistance au choc Charpy (entaillé), +23°C 58[1] kJ/m² ISO 179/1eA
Résistance au choc Izod avec entaille, +23°C 45[1] kJ/m² ISO 180/1A
Résistance au choc Izod avec entaille 70[1] kJ/m² ISO 180/1A
Température -40 °C -
Dureté Shore D 47 - ISO 7619-1
ASTM Data
Module de traction d’élasticité 9.3 MPa ASTM D 638
Résistance de traction à la rupture 11.8 MPa ASTM D 638
Allongement d’élasticité 9 % ASTM D 638
Allongement à la rupture 500 % ASTM D 638
Module de flexion 530 MPa ASTM D 790
Résistance à la flexion 12.8 MPa ASTM D 790
Dureté D Shore 47 - ASTM D 2240
Izod choc avec entaille, 1/4 in 589 J/m ASTM D 256
Izod choc avec entaille, bas température 785 J/m ASTM D 256
Température -40 °C -
1: 4 mm
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 0.45 MPa 65 °C ISO 75-1/-2
Coeffic. de dilatation therm. linéique, parallèle 146 E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 206 E-6/K ISO 11359-1/-2
ASTM Data
coefficient de dilatation thermique, long. 146 E-6/K ASTM D 696
Coefficient de dilatation thermique, trav. 206 E-6/K ASTM D 696
DTUL à 66 psi 71[2] °C ASTM D 648
2: 6.4 mm
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Résistivité transversale 1E14 Ohm*m IEC 62631-3-1
Résistivité superficielle 1E14 Ohm IEC 62631-3-2
ASTM Data
Rigidité diélectrique, peu de temps 25 kV/mm ASTM D 149
Résistance de la surface 1E14 Ohm ASTM D 257
Résistance volumique 1E16 Ohm*cm ASTM D 257
Propriétés diversesValeurUnitéNorme du test
Absorption d'humidité 0.05 % Sim. to ISO 62
Masse volumique 890 kg/m³ ISO 1183
Densité 890 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 70 - 80 °C -
Pré-séchage - temps 3 - 4 h -
L'humidité de traitement ≤0.05 % -
Température de la matière fondue 210 - 240 °C -
Température du moule 40 - 60 °C -
Zone 1 190 - 210 °C -
Zone 2 200 - 230 °C -
Zone 3 200 - 240 °C -
Température de la buse 210 - 230 °C -
Caractéristiques
Transformation
Moulage par injection
Applications
Automobile
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.