Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LUPOY GN1004FA - PC - LG Chem

Material Data Center offers the following functions for LUPOY GN1004FA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Lupoy datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Indice de fluidité, MFI 12 g/10min ASTM D 1238
Température 300 °C -
Charge 1.2 kg -
Retrait au moulage , parallèle 0.0065 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Module de traction d’élasticité 54.9 MPa ASTM D 638
Allongement à la rupture 100 % ASTM D 638
Module de flexion 2158 MPa ASTM D 790
Résistance à la flexion 88.3 MPa ASTM D 790
Dureté Rockwell R 117 - ASTM D 785
Izod choc avec entaille, 1/8 in 589 J/m ASTM D 256
Izod choc avec entaille, bas température 294 J/m ASTM D 256
Température -30 °C -
Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
UL 94 inflammabilité V-0 - UL 94
Épaisseur testée 1.5 mm -
DTUL à 264 psi 125 °C ASTM D 648
Propriétés diversesValeurUnitéNorme du test
Densité 1200 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 100 - 110 °C -
Pré-séchage - temps 3 - 5 h -
L'humidité de traitement ≤0.02 % -
Température de la matière fondue 290 - 310 °C -
Température du moule 80 - 110 °C -
Zone 1 275 - 290 °C -
Zone 2 285 - 305 °C -
Zone 3 290 - 310 °C -
Température de la buse 285 - 305 °C -
Vitesse de rotation de vis 40 - 70 rpm -
Contre-pression 1 - 4 MPa -
Caractéristiques
Transformation
Moulage par injection
Propriétés spéciales
Ignifugé, Sans halogène, Modifié choc
Résistance Chimique
Résistance chimique générale
Applications
IT / Machine de bureau
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.