Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® S ECO 757G BC50 - ASA - INEOS Styrolution

Material Data Center offers the following functions for Luran® S ECO 757G BC50:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Luran® S ECO 757G BC50 acrylonitrile styrene acrylate (ASA) polymer features high surface quality and good impact strength including enhanced colour fastness. The product delivers superior long-term performance when exposed to UV irradiation and additionally provide excellent chemical resistance. Luran® S ECO 757G BC50 provides the best flowability within the product line and is therefore in particular suitable for demanding injection molding geometries. Luran® S ECO 757G BC50 is an ISCC compliant product leading to a substitution of fossil source styrene with ISCC certified bio-attributed styrene.
Carbon Footprint Reduction vs Fossil-Based (3rd party validated): 60 % (ISO 14044)
Attributed Content of ISCC-certified Bio-Circular Sources (min.): 50 %
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 25 cm³/10min ISO 1133
Température 220 °C -
Charge 10 kg -
Retrait au moulage, parallèle 0.6 % ISO 294-4, 2577
Densité du fondu 960 kg/m³ -
Conductivité thermique du fondu 0.206 W/(m K) -
Chaleur spécifique du fondu 2450 J/(kg K) -
Température d'éjection 88 °C -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2400 MPa ISO 527
Contrainte d'écoulement 51 MPa ISO 527
Déformation au seuil d'écoulement 3.3 % ISO 527
Déformation nominale à la rupture 8 % ISO 527
Module de flexion, 23°C 2400 MPa ISO 178
Résistance à la flexion 75 MPa ISO 178
Résistance au choc Charpy (entaillé), +23°C 12 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 3 kJ/m² ISO 179/1eA
Ball indentation hardness 90 MPa ISO 2039-1
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 96 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 101 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 97 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 95 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm HB class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 mm -
Yellow Card disponible oui - -
Inflammabilité pr. épaisseur h HB class IEC 60695-11-10
Epaisseur de l'éprouvette 3.0 mm -
Yellow Card disponible oui - -
Vitesse de combustion, FMVSS, épaisseur 1 mm 25[1] mm/min ISO 3795 (FMVSS 302)
Other Standards[S]
Conductivité thermique, l'état solide 0.0245 W/(m K) DIN 52612-1
1: 2 mm  S: These properties are reported by the producer according standards that are different to our defaults.
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 1.65 % Sim. to ISO 62
Absorption d'humidité 0.35 % Sim. to ISO 62
Masse volumique 1070 kg/m³ ISO 1183
Bulk density 600 kg/m³ -
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 80 °C -
Pré-séchage - temps 2 - 4 h -
Température de la matière fondue 240 - 280 °C -
Température du moule 40 - 80 °C -
Fonctions
Viscosité / Vitesse de cisaillement , Luran® S ECO 757G BC50, ASA, INEOS Styrolution
Contrainte de cisaillement / Vit. de cisaillement , Luran® S ECO 757G BC50, ASA, INEOS Styrolution
Contrainte / Déformation , Luran® S ECO 757G BC50, ASA, INEOS Styrolution
Module sécant / Déformation , Luran® S ECO 757G BC50, ASA, INEOS Styrolution
Contrainte / Déformation (isochrone) 23°C, Luran® S ECO 757G BC50, ASA, INEOS Styrolution
Module de fluage / Temps 23°C, Luran® S ECO 757G BC50, ASA, INEOS Styrolution
Courbe de fluage 23°C, Luran® S ECO 757G BC50, ASA, INEOS Styrolution
Contrainte / Déformation (isochrone) 60°C, Luran® S ECO 757G BC50, ASA, INEOS Styrolution
Module de fluage / Temps 60°C, Luran® S ECO 757G BC50, ASA, INEOS Styrolution
Courbe de fluage 60°C, Luran® S ECO 757G BC50, ASA, INEOS Styrolution
Volume spécifique (pvT) , Luran® S ECO 757G BC50, ASA, INEOS Styrolution
Module de traction / Température , Luran® S ECO 757G BC50, ASA, INEOS Styrolution
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Additifs
Agent de démoulage
Propriétés spéciales
Modifié choc, Stabilisé à la lumière, Stabilisé aux intempéries, Stabilisé à la chaleur
Résistance Chimique
Résistance chimique générale
Certifications
Contient des ressources renouvelables, ISCC Plus
Applications
Électrotechnique et électrique, Sport, Jouets
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America, Proche-Orient/Afrique
Autres informations
Moulages par injection
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 240 - 280°C

Mold temperature, range: 40 - 80°C

Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.