Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® S KR2858G3 - ASA-GF15 - INEOS Styrolution

Material Data Center offers the following functions for Luran® S KR2858G3:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Luran® S KR2858G3 acrylonitrile styrene acrylate (ASA) polymer features high surface quality and good impact strength including enhanced colour fastness. The product delivers superior long-term performance when exposed to UV irradiation and additionally provide excellent chemical resistance. Luran® S KR2858G3 is a 15% glass fiber reinforced ASA grade offering enhanced heat resistance and superior rigidity.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 5 cm³/10min ISO 1133
Température 220 °C -
Charge 10 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 6600 MPa ISO 527
Contrainte à la rupture 110 MPa ISO 527
Déformation à la rupture 2.5 % ISO 527
Résistance au choc Charpy, +23°C 28 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 7 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 5 kJ/m² ISO 179/1eA
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 110 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 115 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 115 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 30 E-6/K ISO 11359-1/-2
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 1.4 % Sim. to ISO 62
Absorption d'humidité 0.3 % Sim. to ISO 62
Masse volumique 1180 kg/m³ ISO 1183
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 80 °C -
Pré-séchage - temps 2 - 4 h -
Température de la matière fondue 240 - 280 °C -
Température du moule 80 - 95 °C -
Fonctions
Viscosité / Vitesse de cisaillement , Luran® S KR2858G3, ASA-GF15, INEOS Styrolution
Contrainte de cisaillement / Vit. de cisaillement , Luran® S KR2858G3, ASA-GF15, INEOS Styrolution
Contrainte / Déformation , Luran® S KR2858G3, ASA-GF15, INEOS Styrolution
Module sécant / Déformation , Luran® S KR2858G3, ASA-GF15, INEOS Styrolution
Module de traction / Température , Luran® S KR2858G3, ASA-GF15, INEOS Styrolution
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Additifs
Agent de démoulage
Propriétés spéciales
Stabilisé à la lumière, Stabilisé aux intempéries, Stabilisé à la chaleur
Disponibilité régionale
Europe, Proche-Orient/Afrique
Autres informations
Moulages par injection
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 240 - 280°C

Mold temperature, range: 40 - 95°C

Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.