Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® ECO 378P BC60 - SAN - INEOS Styrolution

Material Data Center offers the following functions for Luran® ECO 378P BC60:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Luran® ECO 378P is an easy flow grade of SAN with enhanced chemical resistance and mechanical strength. Luran® ECO 378P BC60 is an ISCC compliant product leading to a substitution of fossil source styrene with ISCC certified bio-attributed styrene.
Carbon Footprint Reduction vs Fossil-Based (3rd party validated): 78 % (ISO 14044)
Attributed Content of ISCC-certified Bio-Circular Sources (min.): 60 %
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 20 cm³/10min ISO 1133
Température 220 °C -
Charge 10 kg -
Retrait au moulage, parallèle 0.5 % ISO 294-4, 2577
Conductivité thermique du fondu 0.17 W/(m K) -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 3800 MPa ISO 527
Contrainte à la rupture 75 MPa ISO 527
Déformation à la rupture 3.5 % ISO 527
Module de flexion, 23°C 3730 MPa ISO 178
Résistance à la flexion 135 MPa ISO 178
Résistance au choc Charpy, +23°C 19 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 19 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 2 kJ/m² ISO 179/1eA
Résistance au choc Izod avec entaille, +23°C 2 kJ/m² ISO 180/1A
Ball indentation hardness 175 MPa ISO 2039-1
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fléchissement s/chrg, 1.80 MPa 89 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 101 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 107 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 70 E-6/K ISO 11359-1/-2
Other Standards[S]
Conductivité thermique, l'état solide 0.17 W/(m K) DIN 52612-1
S: These properties are reported by the producer according standards that are different to our defaults.
Propriétés optiquesValeurUnitéNorme du test
ASTM Data
Haze 1 % ASTM D 1003
Lumière á Transmittance 89 % ASTM D 1003
Other Standards[S]
Indice de réfraction 1.56 - ISO 489
S: These properties are reported by the producer according standards that are different to our defaults.
Propriétés diversesValeurUnitéNorme du test
Absorption d'humidité 0.3 % Sim. to ISO 62
Masse volumique 1080 kg/m³ ISO 1183
Bulk density 600 kg/m³ -
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 80 °C -
Pré-séchage - temps 2 - 4 h -
Température de la matière fondue 220 - 260 °C -
Température du moule 40 - 80 °C -
Vitesse d'injection 200 mm/s -
Fonctions
Viscosité / Vitesse de cisaillement , Luran® ECO 378P BC60, SAN, INEOS Styrolution
Contrainte de cisaillement / Vit. de cisaillement , Luran® ECO 378P BC60, SAN, INEOS Styrolution
Module de cisaillement dynamique / Température , Luran® ECO 378P BC60, SAN, INEOS Styrolution
Contrainte / Déformation , Luran® ECO 378P BC60, SAN, INEOS Styrolution
Module sécant / Déformation , Luran® ECO 378P BC60, SAN, INEOS Styrolution
Contrainte / Déformation (isochrone) 23°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Module de fluage / Temps 23°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Courbe de fluage 23°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Contrainte / Déformation (isochrone) 40°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Module de fluage / Temps 40°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Courbe de fluage 40°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Contrainte / Déformation (isochrone) 60°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Module de fluage / Temps 60°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Courbe de fluage 60°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Contrainte / Déformation (isochrone) 80°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Module de fluage / Temps 80°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Courbe de fluage 80°C, Luran® ECO 378P BC60, SAN, INEOS Styrolution
Volume spécifique (pvT) , Luran® ECO 378P BC60, SAN, INEOS Styrolution
Module de traction / Température , Luran® ECO 378P BC60, SAN, INEOS Styrolution
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés
Propriétés spéciales
Stabilisé à la chaleur, Transparent
Résistance Chimique
Résistance chimique générale
Certifications
Contient des ressources renouvelables, Contact alimentaire, ISCC Plus
Applications
Électrotechnique et électrique
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, Proche-Orient/Afrique
Autres informations
Moulages par injection
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Melt temperature, range: 220 - 260°C

Mold temperature, range: 40 - 80°C

Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.