Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Makrolon® 6487 - PC - Covestro Deutschland AG

Material Data Center offers the following functions for Makrolon® 6487:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Makrolon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
  • MVR (300 °C/1.2 kg) 9.0 cm³/10 min
  • flame retardant
  • UL 94V-0/1.5 mm and 5VA/3.0 mm
  • medium viscosity
  • UV stabilized
  • easy release
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 9 cm³/10min ISO 1133
Température 300 °C -
Charge 1.2 kg -
Retrait au moulage, parallèle 0.7 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.8 % ISO 294-4, 2577
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2450 MPa ISO 527
Contrainte d'écoulement 66 MPa ISO 527
Déformation au seuil d'écoulement 6 % ISO 527
Déformation nominale à la rupture >50 % ISO 527
Résistance au choc Charpy, +23°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N kJ/m² ISO 179/1eU
Perforation - force maximum, +23°C 5200 N ISO 6603-2
Perforation - force maximum, -30°C 6000 N ISO 6603-2
Perforation - Energie, +23°C 50 J ISO 6603-2
Perforation - Energie, -30°C 55 J ISO 6603-2
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de transition vitreuse, 10°C/min 141 °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 122 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 134 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 141 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 65 E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 65 E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm V-0 class IEC 60695-11-10
Epaisseur de l'éprouvette 1.5 mm -
Inflammabilité 5V pr. épaisseur h 5VA class IEC 60695-11-20
Epaisseur de l'éprouvette 3.0 mm -
Aptitude à l'allumage 36 % ISO 4589-1/-2
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 3.1 - IEC 62631-2-1
Permittivité relative, 1MHz 3 - IEC 62631-2-1
Facteur de pertes, 100Hz 8 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 90 E-4 IEC 62631-2-1
Résistivité transversale >1E13 Ohm*m IEC 62631-3-1
Résistivité superficielle >1E15 Ohm IEC 62631-3-2
Rigidité diélectrique 34 kV/mm IEC 60243-1
Indice de résistance au cheminement 225 - IEC 60112
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.3 % Sim. to ISO 62
Absorption d'humidité 0.12 % Sim. to ISO 62
Masse volumique 1200 kg/m³ ISO 1183
Préparation et conditionnement des éprouvettesValeurUnitéNorme du test
ISO Data
Injection, température de la matière fondue 300 °C ISO 294
Injection, température du moule 80 °C ISO 294
Injection, vitesse d'injection 200 mm/s ISO 294
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 120 °C -
Pré-séchage - temps 2 - 3 h -
L'humidité de traitement ≤0.02 % -
Température de la matière fondue 280 - 320 °C -
Température du moule 80 - 100 °C -
Fonctions
Viscosité / Vitesse de cisaillement , Makrolon® 6487, PC, Covestro
Contrainte de cisaillement / Vit. de cisaillement , Makrolon® 6487, PC, Covestro
Module de cisaillement dynamique / Température , Makrolon® 6487, PC, Covestro
Contrainte / Déformation , Makrolon® 6487, PC, Covestro
Module sécant / Déformation , Makrolon® 6487, PC, Covestro
Contrainte / Déformation (isochrone) 23°C, Makrolon® 6487, PC, Covestro
Module de fluage / Temps 23°C, Makrolon® 6487, PC, Covestro
Courbe de fluage 23°C, Makrolon® 6487, PC, Covestro
Contrainte / Déformation (isochrone) 40°C, Makrolon® 6487, PC, Covestro
Module de fluage / Temps 40°C, Makrolon® 6487, PC, Covestro
Courbe de fluage 40°C, Makrolon® 6487, PC, Covestro
Contrainte / Déformation (isochrone) 60°C, Makrolon® 6487, PC, Covestro
Module de fluage / Temps 60°C, Makrolon® 6487, PC, Covestro
Courbe de fluage 60°C, Makrolon® 6487, PC, Covestro
Contrainte / Déformation (isochrone) 90°C, Makrolon® 6487, PC, Covestro
Module de fluage / Temps 90°C, Makrolon® 6487, PC, Covestro
Courbe de fluage 90°C, Makrolon® 6487, PC, Covestro
Caractéristiques
Transformation
Moulage par injection, Extrusion (autres)
Conditionnement
Granulés
Additifs
Agent de démoulage
Propriétés spéciales
Ignifugé, Stabilisé à la lumière, Stabilisé aux intempéries
Disponibilité régionale
Autres informations
Moulages par injection
PREPROCESSING
Max. Water content: 0.01 - 0.02 %
Drying temperature: 120 °C
Drying time:
Circulating air drying oven (50 % fresh air) 4-8 h
Fresh air dryer (high speed dryer) 2-4 h
Dry air dryer 2-3 h

PROCESSING
Melt temperature: 280-320 °C
Mold temperature: 80-100 °C

Use open nozzle.
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com