Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NIPLENE F30 AGR HI - PP-GF30 - Soredi S.p.a.

Material Data Center offers the following functions for NIPLENE F30 AGR HI:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Niplene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Indice de fluidité, MFI 3 g/10min ASTM D 1238
Température 230 °C -
Charge 2.16 kg -
Retrait au moulage , parallèle 0.004 mm/mm ASTM D 955
Retrait au moulage, perpendiculaire 0.006 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Résistance de traction à la rupture 90 MPa ASTM D 638
Module de flexion 6000 MPa ASTM D 790
Résistance à la flexion 140 MPa ASTM D 790
Dureté Rockwell R 113 - ASTM D 785
Izod choc avec entaille, 1/8 in 154 J/m ASTM D 256
Izod choc avec entaille, bas température 86.5 J/m ASTM D 256
Température -20 °C -
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Coeffic. de dilatation therm. linéique, perpend. 30 E-6/K ISO 11359-1/-2
ASTM Data
UL 94 inflammabilité HB - UL 94
Épaisseur testée 1.6 mm -
DTUL à 264 psi 158 °C ASTM D 648
Vicat température 146 °C ASTM D 1525
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 1MHz 2.7 - IEC 62631-2-1
Résistivité transversale 1E13 Ohm*m IEC 62631-3-1
Résistivité superficielle 1E14 Ohm IEC 62631-3-2
Rigidité diélectrique 60 kV/mm IEC 60243-1
Propriétés diversesValeurUnitéNorme du test
Absorption d'humidité 0.1 % Sim. to ISO 62
Densité 1120 kg/m³ ASTM D 792
Caractéristiques
Propriétés spéciales
Modifié choc
Caractéristiques
Renforcement couplée chimique, Homopolymère
Disponibilité régionale
Europe
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com